Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is also a PPA resin.Information provided by DuPont Performan.. |
|||
Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
DuPont Performance Polymers Zytel® HTN FE350038 BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFE350038 BK083 is a 33% glass reinforced, heat stabilized, lubricated, hydrolysis resistant high performance polyamide resin, developed for improved structural performance. It is also a P.. |
|||
Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | |
Celanese VECTRA B230 LCP, 30% Specialty
(Unverified Data**) Exceptional strength and stiffness. Suitable for metal replacement applications. Electrically conductive. 30% carbon fiber reinforced.30% carbon fiber,exceptional strength and stiffness, conductiv.. |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA E440i LCP, 42% Mineral / Glass Reinforced
(Unverified Data**) Mineral and glass filled grade with low warp, easy flow and smooth surface apperance.Information provided by Celanese |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA E473i LCP, 32% Mineral / Glass Reinforced
(Unverified Data**) Vectra E473i is a low warp LCP ith easy flow and high temperature capability.Vectra E473i is a low warp LCP with easy flow and high temperature capability.Information provided by Celanese |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA E845i LDS LCP, 40% Mineral / Glass Reinforced
(Unverified Data**) LDS capable LCP with higher DTUL and impactLDS capable LCP with higher DTUL and impactInformation provided by Celanese |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA FIT72 LCP, 35% Mineral / Glass Reinforced
(Unverified Data**) 35% glass and mineral reinforced grade. It offers ultrahigh flowability, low warpage, and good mechanical property. 35% glass and mineral reinforced grade. It offers ultrahigh flowability, low warpa.. |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA J540 LCP, 40% Mineral Reinforced
(Unverified Data**) 40% Mineral filled, high heat resistance.40% Mineral filled, high heat resistance.Information provided by Celanese |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA S135 LCP, 35% Glass Reinforced
(Unverified Data**) 35% glass reinforced Vectra grade with very low outgassing, very high heat deflection temperature (335°C) and stiffness. Typical applications are lampsockets, lensholders for beamers, electrical a.. |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA S540 LCP, 40% Mineral Reinforced
(Unverified Data**) 40% mineral filled grade, low warpage high flow.40% mineral filled grade, low warpage high flow.Information provided by Celanese |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA S625 LCP, 25% Specialty
(Unverified Data**) Low friction and wear resistance.Low friction and wear resistance.Information provided by Celanese |
|||
Dry Time | 6.00 - 24.0 hour | 6.00 - 24.0 hour | |
Unitika C300VN Characteristics: Flame resistant, transparent (flame resistance: UL94 V0, 0.8 mm) High flowInformation provided by Unitika Ltd. |
|||
Dry Time | 6.00 - 24.0 hour | 6.00 - 24.0 hour | |
Unitika P-5001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Dry Time | 6.00 - 24.0 hour | 6.00 - 24.0 hour | |
Unitika UG-100-20 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Dry Time | 6.00 - 24.0 hour | 6.00 - 24.0 hour | |
Unitika P-1001A Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Dry Time | 6.00 - 24.0 hour | 6.00 - 24.0 hour | |
Unitika PT-3020 Characteristics: Dimensional accuracy (planarity) Heat resistance Creep resistance and elasticity RigidityInformation provided by Unitika Ltd. |
|||
Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
DuPont Performance Polymers Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA) Zytel® HTN51G35NOX BK083 is a 35% glass reinforced high performance polyamide resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution. It is also.. |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA E115i LCP, 15% Glass Reinforced 15% glass reinforcedInformation provided by Celanese |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA E463i LCP, 40% Mineral / Glass Reinforced 40% glass/mineral filled exellent flow, low warpage, high heat resistance.Information provided by Celanese |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA FIT70 LCP, 35% Mineral / Glass Reinforced 35% glass and mineral reinforced grade. It offers excellent flowability, low warpage, excellent surface appearance, excellent dimensional stability, and good weldline strength.Information provided b.. |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA S135 LCP, 35% Glass Reinforced 35% glass reinforced Vectra grade with very low outgassing, very high heat deflection temperature (335¦C) and stiffness. Typical applications are lampsockets, lensholders for beamers, electrical a.. |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA S471 LCP, 45% Mineral / Glass Reinforced High flow, High Heat resistance, Low Warpage, for Thick Walled (>0.2mm) or thin ( |
|||
Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | Handling |
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Dry Time | 6.00 - 24.0 hour | 6.00 - 24.0 hour | |
Unitika P-3001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
DuPont Performance Polymers Zytel® HTN 54G35EF NC010 Polyphthalamide (PPA) Zytel® HTN54G35EF NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin, developed for electrical and electronics applications. It is also a PPA r.. |
|||
Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P.. |
|||
Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP)
(Unverified Data**) Xydar G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology. The moldabili.. |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA MLX4243 LCP High heat resistent, mineral filled LCP material with high flow. Material has silver metallic appearance for use in aesthetic metallic effect applications.Information provided by Celanese |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA E488i LCP, Specialty Ultra low warpInformation provided by Celanese |
|||
Dry Time | 6.00 hour | 6.00 hour | |
Celanese VECTRA S475 LCP, 32% Mineral / Glass Reinforced Super High Flow, High heat Resistance and Low Warp for Thin Parts.Information provided by Celanese |