Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Crastin® CE15315 BK010 PBT
(Unverified Data**) Crastin® CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 6.00 mm |
266 °F @Thickness 0.236 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT
(Unverified Data**) Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 2.00 mm |
266 °F @Thickness 0.0787 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9030FR BK851 PBT
(Unverified Data**) Crastin® LW9030FR BK851 is a 30% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9320 BK851 PBT
(Unverified Data**) Crastin® LW9320 BK851 is a 20% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.750 mm |
266 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Crastin® SK605 BK851 PBT
(Unverified Data**) Crastin® SK605 BK851 is a 30% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 6.00 mm |
266 °F @Thickness 0.236 in |
UL 746B |
DuPont Performance Polymers Crastin® SK609 BK851 PBT
(Unverified Data**) Crastin® SK609 BK851 is a 50% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.750 mm |
266 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Crastin® SK609 BK851 PBT
(Unverified Data**) Crastin® SK609 BK851 is a 50% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.850 mm |
266 °F @Thickness 0.0335 in |
UL 746B |
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT
(Unverified Data**) Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=2.00 mm |
266 °F @Thickness >=0.0787 in |
|
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin Description: LUPOY NF 1005F03R, eco-friendly UL94 V0/1.5 mm, is designed for extrusion products. It combines an excellent physical property balance of heat resistance, transparency and impact streng.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=0.750 mm |
266 °F @Thickness >=0.0295 in |
|
LG Chemical Lupoy NF1009F 08R Polycarbonate Resin Description: LUPOY NF 1009F08R, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=3.00 mm |
266 °F @Thickness >=0.118 in |
|
LG Chemical Lupoy NF1009F 08R Polycarbonate Resin Description: LUPOY NF 1009F08R, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=0.750 mm |
266 °F @Thickness >=0.0295 in |
|
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=0.320 mm |
266 °F @Thickness >=0.0126 in |
|
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose Feature: Injection Molding, PPS+GF40%, General PurposeApplication: Pump Units, Motor Units, etc.CAS No. 25212-74-2 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=1.70 mm |
266 °F @Thickness >=0.0669 in |
|
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose Feature: Injection Molding, PPS+GF40%, General PurposeApplication: Pump Units, Motor Units, etc.CAS No. 25212-74-2 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® 27 U Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® FC 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® G4F 22 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® G4F 23 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® G6F 23 R Polycarbonate-30% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® G8F 23 UR Polycarbonate-40% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® MX 1081 Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=1.50 mm |
266 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GP1000MD PC, Light Diffusion Description: Injection Molding, PC, General Purpose, Light DiffusionApplication: IT/OA Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® F 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® FC 19 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.750 mm |
266 °F @Thickness 0.0295 in |
UL746B |
DSM Arnite® TV4 240 PBT-20% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.750 mm |
266 °F @Thickness 0.0295 in |
|
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.830 mm |
266 °F @Thickness 0.0327 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 6.00 mm |
266 °F @Thickness 0.236 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9030 BK851 PBT
(Unverified Data**) Crastin® LW9030 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=3.00 mm |
266 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GP1000ML PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 1.50 mm |
266 °F @Thickness 0.0591 in |
UL746B |
DSM Arnite® T06 202 PBT (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |