Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Nylene® Vexel™ B50U , High Flow, Un-reinforced PBT Description: Vexel™ B50U is a high flow, un-reinforced PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporatio.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Asia Pacific) Thermoplastic Polyimide Extem* XH1015 Resin. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D 792 |
RTP Company RTP 300 TFE 15 FR Polycarbonate (PC), PTFE Lubricated - Flame Retardant |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Celanese Celanex® 2003HR PBT
(Unverified Data**) Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityHydrolytically stable / injectionInformation provided b.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D 792 |
RTP Company RTP 727 High Density Polyethylene (HDPE), Talc |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R264AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
RTP Company RTP 205D UV Nylon 6/12 (PA 6/12) Glass Fiber 30% - UV Stable
(discontinued **) Glass Fiber 30% - UV StableComments:Glass FiberUV StabilizedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
RTP Company RTP 205D Z Nylon 6/12 (PA 6/12) Glass Fiber 30% - FDA Type
(discontinued **)&l Glass Fiber 30% - FDA TypeComments:Glass FiberFDA CompliantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided .. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-8382 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Highly dimensionally stable at ele.. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 800-21/9-IS-RG Coke PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina 861-40/36-IS-RG Green PVC Compound PVC compound recommended for rolled mill of notebook covering.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 - 1.37 g/cc | 1.31 - 1.37 g/cc | ASTM D 792 |
Karina E 786-10/332-IS-RG Compound PVC White White rigid for spiral hoses (non-toxic)Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC3508 PPE+HIPS (Europe-Africa-Middle East) PRELIMINARY DATA. LNP* Stat-kon* Noryl_NC3508 compound is a 33% glass/mineral/carbon filled PPE+PS. ESD, high heat, tight tolerance: electronic packaging/chip trays. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Teknor Apex APEX® 3610-80 Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: First Generation SeriesInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Teknor Apex APEX® 80853-C Polyvinyl Chloride, Flexible Notes: 105°C, Non-lead Stabilized, Insulation; PVC Insulation intended for use in 90°C wet locations; RoHS CompliantFeatures: Flame Retardant; Oil Resistant Uses: Insulation; Wet Rated Insulat.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | |
Teknor Apex Elexar® EL 1934C Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D 792 |
RTP Company ESD A 2180 Polyetherimide (PEI), Carbon Fiber - ESD Protection - Static Dissipative |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Blue LL40445/2 Concentrate Based In LLDPE DescriptionPOLYBATCH® LL40445/2 is a blue color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® LL40445/2 is typic.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | |
Trelleborg R448 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D 792 |
RTP Company RTP 2599 X 131264 A Polycarbonate/ABS Alloy (PC/ABS), Fiber Reinforced - Electrically Conductive - EMI/RFI Shielding |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D 792 |
RTP Company RTP 283 TFE 15 SI 2 Nylon 6/6 (PA), Carbon Fiber - PTFE Lubricated - Silicone Lubricated |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SIM 6029 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | |
Colorite Polymers 9811 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Celanese CELANEX 1602Z PBT, Unfilled Celanex 1602Z is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1602Z has an internal lubricant.Information provi.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Asahi Kasei Thermofil P6-9900-0570 Unfilled, Flame Retardant, Heat Stabilized Information provided by Asahi Thermofil |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | |
Aremco Corr-Paint™ CP4050 High Temperature Protective Coating Silicone Low viscosity, green coating for power resistors to 1100°F (593°C) |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Celanese Celanex® 1600FC PBT
(Unverified Data**) Celanex 1600FC is a high molecular weight grade of unreinforced polybutylene terephthalate for use in food contact applications that can be used in both extrusion and injection molding applications... |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
Celanese Celanex® 2002-2 PBT
(Unverified Data**) Celanex 2002-2 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-2 ia a medium flow material that contains a.. |
|||
Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
PolyOne Edgetek® AM-30CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |