Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 130 °C @Thickness 6.00 mm |
266 °F @Thickness 0.236 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT
(Unverified Data**) Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.750 mm |
266 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Crastin® SK603 BK851 PBT
(Unverified Data**) Crastin® SK603 BK851 is a 20% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Crastin® SK605 BK851 PBT
(Unverified Data**) Crastin® SK605 BK851 is a 30% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.750 mm |
266 °F @Thickness 0.0295 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.750 mm |
266 °F @Thickness 0.0295 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=3.00 mm |
266 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GP1000HU PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: Electric & Electronic (Housing, Components) For Suit caseCAS: 103598-77-2Information provided by LG Chemic.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=3.00 mm |
266 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GP1000L PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, E&E Housing and Components Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=2.00 mm |
266 °F @Thickness >=0.0787 in |
|
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin Description: LUPOY NF 1005F03R, eco-friendly UL94 V0/1.5 mm, is designed for extrusion products. It combines an excellent physical property balance of heat resistance, transparency and impact streng.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=2.00 mm |
266 °F @Thickness >=0.0787 in |
|
LG Chemical Lupoy NF1009F 08R Polycarbonate Resin Description: LUPOY NF 1009F08R, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=0.750 mm |
266 °F @Thickness >=0.0295 in |
|
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=3.00 mm |
266 °F @Thickness >=0.118 in |
|
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose Feature: Injection Molding, PPS+GF40%, General PurposeApplication: Pump Units, Motor Units, etc.CAS No. 25212-74-2 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® 18 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® 18 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® 19 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® 22 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® FC 19 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® MX 1081 Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=3.00 mm |
266 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GP1000LS PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, Electric & Electronic Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=3.00 mm |
266 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GP1000M PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA, Electric & Electronic Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provide.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=1.50 mm |
266 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GP1000MD PC, Light Diffusion Description: Injection Molding, PC, General Purpose, Light DiffusionApplication: IT/OA Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=1.50 mm |
266 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GP1000MR PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=3.00 mm |
266 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GP1000MR PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® MX 2015 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 1.50 mm |
266 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K222-KGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.800 mm |
266 °F @Thickness 0.0315 in |
|
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 1.50 mm |
266 °F @Thickness 0.0591 in |
|
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.800 mm |
266 °F @Thickness 0.0315 in |
UL 746B |
DuPont Performance Polymers Crastin® T835FRUV NC010 PBT Crastin® T835FRUV NC010 is a 5% glass fiber reinforced, toughened, flame retardant polybutylene terephthalate resin for injection molding. (precommercial code = Crastin® CE2402)Information provide.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9030 BK851 PBT
(Unverified Data**) Crastin® LW9030 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® F 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |