Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 300 - 310 °C | 572 - 590 °F | |
Oceanchem Group Decabromodiphenyl Oxide (DECA/DBDPO) Molecular Formula: C12Br10OCas No.: 1163-19-5Characteristics: White powder, no poison, no smell and noncorrosion. Indissolvable in water, ethyl alcohol, acetone, benzene, arene chloride.Use: It is .. |
|||
Melting Point | 300 - 323 °C | 572 - 613 °F | Average value: 313 °C Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Melting Point | 300 °C | 572 °F | DAM; ASTM D3418 |
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
Melting Point | 300 °C | 572 °F | 10°C/min, First Heat; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym.. |
|||
Melting Point | 300 °C | 572 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Melting Point | 300 °C | 572 °F | ASTM D3418 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Melting Point | >= 300 °C | >= 572 °F | |
Solvay Specialty Polymers Hyflon® PFA 450 Fluoropolymer
(discontinued **) Data provided by the manufacturer.Hyflon® PFA 450 has outstanding physical and chemical properties typical of fluoropolymers.Hyflon® PFA 420 |
|||
Melting Point | 300 - 315 °C | 572 - 599 °F | Average value: 307 °C Grade Count:16 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Melting Point | 300 - 320 °C | 572 - 608 °F | |
Indium Corp. Indalloy 168 Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ G1301A-M61 Nylon, 30% Glass Filled 30% Glass reinforced and impact modified injection grade.Main Features:Higher elongation and impact strengthHeat resistanceChemical resistanceExample of applications:Quick connector |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ G1350A-M42 Nylon, 35% Glass Filled 35% Glass reinforced injection grade. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment.Main Features:Hydrolysis resistanceHeat resista.. |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ N1000A-M41 Nylon Standard unreinforced injection grade. Main features:Low water absorptionChemical ResistanceExamples of application are:Friction and wear applicationGear and Wheel |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ N1001A-M41 Nylon Low friction unreinforced injection grade. Main Features:Low friction coefficientHigh impact strengthExamples of applications are:Friction and wear applicationGear and wheel |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ N1002A-M41 Nylon Low friction unreinforced injection grade. Main Features:Low friction coefficientLow wearExamples of applications are:Friction and wear applicationGear and wheel |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | |
Guarniflon PFA Perfluoroalkoxy Polymer Fluorinated thermoplastic material, offers the advantages of being thermo-processed whilst at the same time having the properties of PTFE, with excellent chemical and mechanical resistance for appli.. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | DSC |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | DSC |
Solvay Specialty Polymers Hyflon® PFA P7010 Perfluoroalkoxy (PFA) Hyflon® PFA P7010 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in anti.. |
|||
Melting Point | 300 °C | 572 °F | |
Williams Advanced Alloys WS300 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 300 - 315 °C | 572 - 599 °F | |
Zeus PFA Tubing PFA, or perfluoroalkoxy, is well recognized for its ability to maintain mechanical integrity in extreme temperatures even when exposed to caustic chemicals. PFA comes in high purity versions that ar.. |
|||
Melting Point | 300 °C | 572 °F | DAM; first heat; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR NC010 is a 35% glass reinforced toughened heat stabilized lubricated high performance polyamide resin. It is also a P.. |
|||
Melting Point | 300 °C | 572 °F | DAM; first heat; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® HTN FE8200 BK431 Polyphthalamide (PPA)
(Unverified Data**) Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 BK431 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also.. |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® XE 4216 black 9233 PA6T/66-GF30 Product description: Grivory XE 4216 black 9233 is a high heat stabilized, 30% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection molding. Polymer designation .. |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® XE 4217 black 9233 PA6T/66-GF45 Product description: Grivory XE 4217 black 9233 is a high heat stabilized, 45% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection moulding. Polymer designation.. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | |
Asahi Glass Fluon® P-62XP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | |
Asahi Glass Fluon® P-830UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | ASTM D3307 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Melting Point | 300 °C | 572 °F | 10°C/min, First Heat; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
Melting Point | 300 °C | 572 °F | 10°C/min, First Heat; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® HTN FE8200 BK431 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFE8200 BK431 is an unreinforced, toughened, heat stabilized, lubricated high performance polyamide resin for injection molding. It is also a PPA resin.Information provided by DuPont Perfo.. |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestar™ G1300A-M41 Nylon, 30% Glass Filled Glass reinforced injection grade. Main Features:Chemical resistanceHeat resistanceExamples of applications:Gears and bearing retainersIntercooler tank and turbo duct pipe |