Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Talc Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 2121UV-M-31 is a 30% black filled polypropylene homopolymer. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.10 - 1.16 g/cc
1.10 - 1.16 g/cc
ASTM D792
Melt Flow 9.0 - 14 g/10 min

@Temperature 230 °C
9.0 - 14 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R >= 88
>= 88
ASTM D785
Tensile Strength, Yield >= 26.2 MPa
>= 3800 psi
2 in/min; ASTM D638
Elongation at Break >= 3.0 %
>= 3.0 %
ASTM D638
Flexural Modulus >= 2.84 GPa
>= 412 ksi
ASTM D790
Izod Impact, Notched 0.149 J/cm
0.280 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) >= 115 °C
>= 239 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) >= 80.0 °C
>= 176 °F
ASTM D648