Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 16.5 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 16.5 kV/mm
419 kV/in
dry; IEC 60243-1
Murtfeldt Murytal® C Blue [FS] Acetal Copolymer
Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th..
Dielectric Strength 16.5 kV/mm
420 kV/in
Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite
Formerly known as grade MM 1100. Synthetic mica filler. Does not burn. Excellent radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating m..
Dielectric Strength 16.5 kV/mm
419 kV/in
Momentive Performance Materials RTV5223 Neutral Cure, One Component RTV Adhesive Sealant
RTV5220 series sealants are alkoxy neutral cure, one-component, ready to use silicone adhesive sealants exhibiting low modulus/high elongation that will maintain a strong bond even when exposed to e..
Dielectric Strength 16.5 kV/mm
419 kV/in
NF EN 60243.1
Isoflon Tisoflon® 14 AD Polytetrafluoroethylene Coated Glass Fabric
PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon.
Dielectric Strength 16.5 kV/mm
419 kV/in
Momentive Performance Materials RTV5229 Gray Adhesive Sealant, Low Modulus Paste
One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Economical true neu..
Dielectric Strength 16.5 kV/mm
419 kV/in
Schott D 263 Thin Borosilicate Glass
D 263 is a low alkali borosilicate glass that is produced by melting the purest raw materials. As such, it is very resistant to chemical attack. D 263, with its specific properties and large rang..
Dielectric Strength 16.5 kV/mm
420 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Elastoblend® PA6 IM 409 L MB
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc.
Dielectric Strength 16.5 kV/mm
420 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Elastoblend® PA6 IM 811 HS L (Dry)
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedTPCI# 6109102Information provided by TP Comp..
Dielectric Strength 16.5 kV/mm
420 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Elastoblend® PA6 IM HS L
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc.
Dielectric Strength 16.5 kV/mm
420 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Elastoblend® PA6 IM L W
Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc..
Dielectric Strength 16.5 kV/mm
420 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® PA6 GF30 L 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation p..
Dielectric Strength 16.5 kV/mm
420 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® PA6 GF33 HS YL030 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and SoftAppearance: YellowInformation..
Dielectric Strength 16.5 kV/mm
420 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Plastiblend® PA6/ABS 1120 GF20 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: Natural ColorInformation p..
Dielectric Strength 16.5 kV/mm
420 kV/in
ASTM D149
Styron CALIBREâ„¢ 301-10 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Dielectric Strength 16.5 kV/mm
420 kV/in
ASTM D149
Styron CALIBREâ„¢ 301-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Dielectric Strength 16.5 kV/mm
419 kV/in
Styron CALIBREâ„¢ MEGARAD 2080 10 Polycarbonate, Gamma Radiation Resistant
CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g..
Dielectric Strength 16.5 kV/mm
420 kV/in
ASTM D149
Styron EMERGEâ„¢ 4310-22 Polycarbonate
EMERGEâ„¢ PC 4310-22 advanced resin is high-performance polycarbonate resin offering high heat resistance, toughness, and superior flow. Applications: Consumer Electronics and Information Techn..
Dielectric Strength 16.5 kV/mm
420 kV/in
ASTM D149
Styron CALIBREâ„¢ 301 EP Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Dielectric Strength 16.5 kV/mm
420 kV/in
ASTM D149
Styron CALIBREâ„¢ 302-06 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Dielectric Strength 16.5 kV/mm
420 kV/in
ASTM D149
Styron CALIBREâ„¢ 303-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Dielectric Strength 16.5 kV/mm
420 kV/in
ASTM D149
Styron EMERGEâ„¢ 4310-15 Polycarbonate
EMERGEâ„¢ PC 4310-15 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq..
Dielectric Strength 16.5 kV/mm
420 kV/in
Tra-Con Tra-Bond FDA12 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA12 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admin..
Dielectric Strength 16.5 kV/mm
420 kV/in
Tra-Con Tra-Bond FDA22 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA-22 is a high viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admini..
Dielectric Strength 16.5 kV/mm
420 kV/in
Tra-Con Tra-Bond FDA23 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA-23 is a high viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admini..
Dielectric Strength 16.5 kV/mm
420 kV/in
ASTM D149
AdvanSource Biomaterials ChronoFlex® C 75D Biodurable Medical Grade Polyurethane
ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome..
Dielectric Strength 16.5 kV/mm
420 kV/in
short term; ASTM D149
Celanese CELANEX 2000-3 PBT, Unfilled
Celanex 2000-3 is a general purpose, unreinforced PBT with a good balance of mechanical properties and processabillity.. Celanex 2000-3 is a high flow material. Celanex 2000-3 contains an internal..
Dielectric Strength 16.5 kV/mm
420 kV/in
short term; ASTM D149
Celanese CELANEX 2002-2 PBT, Unfilled
Celanex 2002-2 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-2 ia a medium flow material that contains a..
Dielectric Strength 16.5 kV/mm
420 kV/in
short term; ASTM D149
Celanese Celanex® 602AC PBT, Glass Reinforced
Celanex 602AC is a 10% fiberglass reinforced PBT that has lower warpage and improved impact over standard PBT.To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a ..
Dielectric Strength 16.5 kV/mm
420 kV/in
S/T; ASTM D149
RTP Company RTP 1703  Modified Polyphenylene Oxide (PPO) Glass Fiber 20%  (discontinued **)&
Glass Fiber 20%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Dielectric Strength 16.5 - 18.0 kV/mm
420 - 457 kV/in
Average value: 17.6 kV/mm Grade Count:4
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and ..