DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Zytel® EFE7374 is a 40% fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for injection molding. It has an improved impact resistance and excellent surface appearance and gloss.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
DAM; ISO 1183
Water Absorption 1.7 %
<br>@Temperature 23.0 °C
1.7 %
<br>@Temperature 73.4 °F
Equilibrium 50%RH; DAM; ISO 62, Similar to
5.4 %
<br>@Temperature 23.0 °C
5.4 %
<br>@Temperature 73.4 °F
Saturation, immersed; DAM; ISO 62, Similar to
Linear Mold Shrinkage, Flow 0.0020 cm/cm
<br>@Thickness 2.00 mm
0.0020 in/in
<br>@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
<br>@Thickness 2.00 mm
0.0060 in/in
<br>@Thickness 0.0787 in
DAM; ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 128 MPa
<br>@Temperature 23.0 °C
18600 psi
<br>@Temperature 73.4 °F
50%RH; ISO 527
185 MPa
<br>@Temperature 23.0 °C
26800 psi
<br>@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break 3.5 %
<br>@Temperature 23.0 °C
3.5 %
<br>@Temperature 73.4 °F
DAM; ISO 527
7.3 %
<br>@Temperature 23.0 °C
7.3 %
<br>@Temperature 73.4 °F
50%RH; ISO 527
Elongation at Yield 5.0 %
<br>@Temperature 23.0 °C
5.0 %
<br>@Temperature 73.4 °F
DAM; ISO 527
22 %
<br>@Temperature 23.0 °C
22 %
<br>@Temperature 73.4 °F
50%RH; ISO 527
Tensile Modulus 7.50 GPa
<br>@Temperature 23.0 °C
1090 ksi
<br>@Temperature 73.4 °F
50%RH; ISO 527
12.2 GPa
<br>@Temperature 23.0 °C
1770 ksi
<br>@Temperature 73.4 °F
DAM; ISO 527
Izod Impact, Notched (ISO) 18.0 kJ/m²
<br>@Temperature -30.0 °C
8.57 ft-lb/in²
<br>@Temperature -22.0 °F
50%RH; ISO 180/1A
19.0 kJ/m²
<br>@Temperature -30.0 °C
9.04 ft-lb/in²
<br>@Temperature -22.0 °F
DAM; ISO 180/1A
24.0 kJ/m²
<br>@Temperature 23.0 °C
11.4 ft-lb/in²
<br>@Temperature 73.4 °F
DAM; ISO 180/1A
30.0 kJ/m²
<br>@Temperature 23.0 °C
14.3 ft-lb/in²
<br>@Temperature 73.4 °F
50%RH; ISO 180/1A
Charpy Impact Unnotched 10.5 J/cm²
<br>@Temperature -30.0 °C
50.0 ft-lb/in²
<br>@Temperature -22.0 °F
50%RH; ISO 179/1eU
11.0 J/cm²
<br>@Temperature 23.0 °C
52.3 ft-lb/in²
<br>@Temperature 73.4 °F
DAM; ISO 179/1eU
11.3 J/cm²
<br>@Temperature 23.0 °C
53.8 ft-lb/in²
<br>@Temperature 73.4 °F
50%RH; ISO 179/1eU
11.8 J/cm²
<br>@Temperature -30.0 °C
56.1 ft-lb/in²
<br>@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 1.70 J/cm²
<br>@Temperature -30.0 °C
8.09 ft-lb/in²
<br>@Temperature -22.0 °F
DAM; ISO 179/1eA
1.80 J/cm²
<br>@Temperature -30.0 °C
8.57 ft-lb/in²
<br>@Temperature -22.0 °F
50%RH; ISO 179/1eA
2.40 J/cm²
<br>@Temperature 23.0 °C
11.4 ft-lb/in²
<br>@Temperature 73.4 °F
DAM; ISO 179/1eA
3.30 J/cm²
<br>@Temperature 23.0 °C
15.7 ft-lb/in²
<br>@Temperature 73.4 °F
50%RH; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 212 °C
414 °F
DAM; ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 270 °C
518 °F
DAM; Optimum
260 - 280 °C
500 - 536 °F
DAM
Mold Temperature 50.0 - 100 °C
122 - 212 °F
DAM
80.0 °C
176 °F
DAM; optimum
Drying Temperature 80.0 °C
176 °F
DAM
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM
Moisture Content <= 0.20 %
<= 0.20 %
DAM
Descriptive Properties Value Comments
Forms Pellets
DAM
Generic PA66
DAM
Material Status Preliminary Data
DAM
Processing Method Injection Molding
DAM
Product Category Toughened Resins
DAM
RoHS Compliance Contact Manufacturer
DAM