Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
SABIC P5510 Black High Density Polyethylene for Pipes Product Description: P5510 is a black compound high density (class MRS 8 - PE 80) polyethylene with bimodal distribution of molecular mass. It is specifically designed for Pressure Pipe applicatio.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1483T PC Copolymer Lexan* EXL1483T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release, transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility i.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1493T PC Copolymer Lexan* EXL1493T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance, with mold release. This resin offers excellent low temperature (-3.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 HI Polyamide 6, Impacted FeaturesPA 6 with the content of thermoplastic elastomer. Impacted, for mouldings with high toughness either at low temperatures, suitable for external use, eg. ski shoes, sports and safety helmets.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East) XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East) XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6
(Unverified Data**) Zytel® 73G45 BK263 is a 45% glass fiber reinforced, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) Zytel® EFE7374 is a 40% fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for injection molding. It has an improved impact resistance and excellent surface appearance and gloss.I.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -20.0 °C |
11.4 ft-lb/in² @Temperature -4.00 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Zytel® ST7301 NC010 is a Super Tough, heat stabilized, lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and humidity.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eA |
Styron Magnumâ„¢ 3513 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3513 is a grade which combines high impact with good flowability. It is suitable for injection molding and extrusion applications.Information provided by DowThis product line was spun .. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Sax Polymers SAXLAC 320 Acrylonitrile Butadiene Styrene Saxalac 320 is a high impact resistant, easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Sax Polymers SAXLAC 320A Acrylonitrile Butadiene Styrene Saxalac 320A is an antistatic, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.I.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Sax Polymers SAXLAC 320U Acrylonitrile Butadiene Styrene Saxalac 320U is an UV protected, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Polyram Polytron P40N03 Polypropylene, 40% Long Glass Fibers Is a chemically coupled 40% long glass fibers reinforced natural polypropylene, heat stabilized, for injection molding applications. These products have significantly improved impact performance ch.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis Xmod™ GD302HP Polypropylene, Glass Fiber Reinforced Xmod™ GD302HP is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material has an excellent balance between impact stre.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Novamid® 1015G35 NAT PA6-GF35 35% Glass Reinforced, Injection Molding |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Novamid® 1015GH35 BK37 PA6-GF35 35% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, Conditioned Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultrason® P 3010 MR SW 10101 PPSU Description: Unreinforced, higher viscosity injection molding grade, flame retardant and with improved chemical resistance. This grade is black colored and demolding optimized. Abbreviated designati.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eA |
Eurotec® Tecomid® NB40 GR30 NL IH PA 6 30% glass fiber reinforced, impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, Conditioned Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Stanyl® TS200F10 PA46-GF50 50% Glass Reinforced |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East) High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |