A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 90 g/10 min

@Load 2.16 kg,
Temperature 230 °C
90 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4210 psi
2 in/min; ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus 1.30 GPa
189 ksi
ASTM D790
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 160 °C
320 °F