Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dry Time = 2.00 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Dry Time 2.00 - 3.00 hour
2.00 - 3.00 hour
PolyOne OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE)
OnFlex™ HFFR 315-01 a is non-halogen flame retardant material designed for flexible power cord insulation, cable jackets, and ribbon cables. New Product. Commercial specifications have not been est..
Dry Time 2.00 hour
2.00 hour
PolyOne OnFlex™ S HF 60A-3S1982 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Dry Time 2.00 hour
2.00 hour
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy)
Information provided by PolyOne
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT  (Unverified Data**)
Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0..
Dry Time 2.00 - 3.00 hour
2.00 - 3.00 hour
Blow Molding
DuPont Performance Polymers Hytrel® HTR8730 BK320 TPC-ET  (Unverified Data**)
Hytrel® HTR8730 BK320 is a high viscosity thermoplastic polyester elastomer designed for blow molding. It has excellent mechanical properties at elevated temperatures and very good resistance to mo..
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Pasargad Polymer Peyvand Pasamid 3P-H1000B Nylon 6
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM
DuPont Performance Polymers Zytel® 101L BKB009 Nylon 66  (Unverified Data**)
Zytel® 101L BKB009 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66  (Unverified Data**)
Zytel® 70G30HSL BK039B is a 30% glass reinforced, heat stabilized, black nylon 66 resin for injection molding.Information provided by DuPont Performance Polymers
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM; Dehumidified Dryer; Injection Molding
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6  (Unverified Data**)
Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h..
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Injection Molding
LG Chemical AF312 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Injection Molding
LG Chemical AF345 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi..
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Injection Molding
LG Chemical ALPHALAC SF510 HIPS
Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa..
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Injection Molding
LG Chemical HIPS MI770 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
Dry Time 2.00 - 6.00 hour
2.00 - 6.00 hour
Gromax BFG45-B100N1 Nylon 6 46% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Dry Time 2.00 - 6.00 hour

@Temperature 80.0 °C
2.00 - 6.00 hour

@Temperature 176 °F
Lanxess Durethan® BKY 115 H3.0 DUS008 Nylon 6, 15% Glass Fiber
PA 6, 15% glass fibers, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS.
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DuPont Performance Polymers Crastin® S600LF NC010 PBT
Crastin® S600LF NC010 is an unreinforced, Teflon® PTFE powder lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Eurotec® Tecodur® PB70 NL PBT, unfilled, natural
Information provided by Eurotec®
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Eurotec® Tecomid® NA40 GR40 NL RM PA6.6, 40% glass fiber reinforced, MoS2 modified, natural
Information provided by Eurotec®
Dry Time 2.00 hour
2.00 hour
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Dry, 60% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Celanese Celstran® PA66-GF50-0111P10/11 PA666, 50% Glass Reinforced
Material code according to ISO 1043-1: PA66PA66/6 Copolymer with 50% reinforced long glass fiber, high gloss, UL - listing (f1)Information provided by Celanese
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Handling
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Handling
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester
Dry Time 2.00 hour
2.00 hour
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Dry, 25% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Dry Time 2.00 hour
2.00 hour
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Dry Time 2.00 hour
2.00 hour
Celanese Celstran® PP-GF30-02 AD 3019 PP, 30% Glass Reinforced
30% long glass fiber reinforced polypropylene - UV stabilizedInformation provided by Celanese
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Celanese Celstran® PA66-GF50-0111P7.5/11 PA666, 50% Glass Reinforced
Material code according to ISO 1043-1: PA66PA66/6 copolymer with 50% ash content - 7.5mmInformation provided by Celanese
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Celanese Celstran® PA66-SF6-02 PA66, 6% Stainless Steel Reinforced
6% stainless steel reinforced nylon 6/66% stainless steel fiber reinforced, heat stabilized nylon 6/6Celstran can be processed on a standard injection molding unit.Information provided by Celanese
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Injection Molding
LG Chemical HF350U ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical
Dry Time 2.00 - 3.00 hour
2.00 - 3.00 hour
Injection Molding
LG Chemical LI912 ASA
Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66  (Unverified Data**)
Zytel® 70G35HSRX BK099 a 35% glass reinforced, heat stabilized, hydrolysis resistant PA66 for injection molding. Developed for applications designed for direct overmolding of gaskets onto thermopla..
Copyright © lookpolymers.com All Rights Reserved