Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 10.5 J/cm² @Temperature -20.0 °C |
50.0 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PQ 81 T 30 PP, 30% mineral filling FeaturesModified PP for injection moulding with the content of 30% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6/66 GF 50 PA6/66, 50% glass fibre FeaturesPA 6/66 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-g.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID® 6 GF 40 HI PA6 reinforced with glass fiber, improved impact strength PA 6 for injection molding, reinforced with 40% glass fiber, impact modified. Application: impacted moldings and moldings with higher strength applied in automotive, electrical, engineering and cons.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® S223-G8U (Cond.) 43% Glass Reinforced Nylon 66 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-G3U (Cond.) 15% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-PG6U (Dry) 33% Glass Reinforced, Impact Modified Nylon 6 (North America)
(discontinued **)&l Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature -30.0 °C |
50.0 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) Zytel® EFE7374 is a 40% fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for injection molding. It has an improved impact resistance and excellent surface appearance and gloss.I.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Lanxess Durethan® BKV 140 DUS008 000000 Nylon 6, 40% Glass Fiber PA 6, 40% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 179-1eU |
Lanxess Durethan® BKV 140 H2.0 DUS008 900051 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 40% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature -30.0 °C |
50.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Durethan® DP AKV 50 HR H2.0 901510 Nylon 66, 50% Glass Fiber PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance, and hydrolysis resistanceApplication Examples: coolant manifolds |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® DP AKV 50 HR H2.0 901510 Nylon 66, 50% Glass Fiber PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance, and hydrolysis resistanceApplication Examples: coolant manifolds |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-G0 (Cond.) 50% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-G0 Nylon 6-50% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-G4U (Cond.) 23% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-PG6 Impact Modified Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-PG8 (Cond.) 40% Glass Reinforced, Impact Modified Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-PG8 (Dry) 40% Glass Reinforced, Impact Modified Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-PG8 Impact Modified Nylon 6-40% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® S223-HG7 (Cond.) 35% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® S223-HG7 Nylon 66-35% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
DSM Stanyl® OCD2100 BK27021 PA46-GF40 40% Glass Reinforced, Heat Stabilized |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
Eurotec® Tecomid® NB40 GR50 NL PA 6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature -30.0 °C |
50.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Dry) Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature -30.0 °C |
50.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature -30.0 °C |
50.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultramid® KR 4350 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature -30.0 °C |
50.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature -30.0 °C |
50.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-PG8 Impact Modified Nylon 6-40% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 10.5 J/cm² @Temperature 23.0 °C |
50.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
Eurotec® Tecomid® NB40 GR30 NL IH PA 6 30% glass fiber reinforced, impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |