Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PQ 81 T 25 PP, 25% mineral filling FeaturesModified PP for injection moulding with the content of 25% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shri nkage. Gen.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 GF 50 LS PA6, 50% glass fibre, light stability FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -20.0 °C |
8.57 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 65/1M PA6 reinforced with 65% glass fibre Features: PA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
PolyOne OnFlex™ BIO 5180D-E0014 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® G360 ABS (Europe-Africa-Middle East) CYCOLAC G360 is a high flow, high impact, medium to high heat resistant injection moulding ABS grade. It is recommended for large or complex parts in the automotive or electrical power tool segments.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Thickness 102 mm, Temperature -20.0 °C |
8.57 ft-lb/in² @Thickness 4.00 in, Temperature -4.00 °F |
ISO 179 |
Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANAMID 66 A33^E F30 Nylon 66, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -20.0 °C |
8.57 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANFILL BOTTLE BY45C2 Blow Molding Grade Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANMID 6 B43^ D F15 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A RV300 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 50 Polyamide 6, 50% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® E41HSB NC010 Nylon 66
(Unverified Data**) Zytel® E41HSB is an unreinforced, high viscosity, heat stabilized polyamide 66 for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) Zytel® EFE7374 is a 40% fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for injection molding. It has an improved impact resistance and excellent surface appearance and gloss.I.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
LG Chemical HI-121 ABS, High Impact Feature: Injection Molding, Well Balanced Mechanical PropertiesApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information Provided by LG Chem |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
LG Chemical LG-703A ABS, Low Gloss, General Purpose Information Provided by LG Chem |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Lanxess Durethan® BKV 130 H3.0 101006 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30 H3.0, ev.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Solvay TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, Conditioned Description: TECHNYL® eXten D 238 V30 is a PA6,10 30% glass fiber reinforced and impact modified suitable for injection molding. TECHNYL® eXten D 238 V30 is based on a partially bio-sourced po.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Sax Polymers SAXAMID 136F4Q32 Nylon 6, 20% Glass Fiber SAXAMID 136F4Q32 is a high impact-modified polyamide 6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polyram PlusTek PA313G43 Nylon 66 for Injection Molding, 43% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 43% Glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Akulon® K224-G8 PA6-GF40 40% Glass Reinforced |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-HG7 (Dry) 35% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Thickness 3.00 mm, Temperature -30.0 °C |
8.57 ft-lb/in² @Thickness 0.118 in, Temperature -22.0 °F |
complete break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 3100 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Hytrel® DYM1300 BK320 TPC-ET
(Unverified Data**) Hytrel® DYM1300 is a high performance thermoplastic elastomer with high modulus, suited for air bag door applications.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -40.0 °C |
8.57 ft-lb/in² @Temperature -40.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K224-PG8 Impact Modified Nylon 6-40% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -40.0 °C |
8.57 ft-lb/in² @Temperature -40.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Charpy Impact, Notched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® VX3608C PBT (Europe-Africa-Middle East) VALOX VX3608C is an impact modified, flame retardant PBT+PC injection moulding resin. Application: electrical enclosures. This grade is 3607U with reduced oxygen index.This data was supplied by SABI.. |