Mechanical Properties Metric English Comments
Tensile Strength at Break 185 MPa

@Temperature 23.0 °C
26800 psi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
Tensile Strength at Break 185 MPa

@Temperature 23.0 °C
26800 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL NC010 is a 30% glass fiber reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 185 MPa

@Temperature 23.0 °C
26800 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6  (Unverified Data**)
Zytel® EFE7374 is a 40% fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for injection molding. It has an improved impact resistance and excellent surface appearance and gloss.I..
Tensile Strength at Break 185 MPa

@Temperature 90.0 °C
26800 psi

@Temperature 194 °F
LATI Laramid G/50 PPA, 50% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Strength at Break 185 MPa

@Temperature 23.0 °C
26800 psi

@Temperature 73.4 °F
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 185 MPa

@Temperature 23.0 °C
26800 psi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Strength at Break 185 MPa

@Temperature 23.0 °C
26800 psi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/35-V0KB1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Strength at Break 185 MPa

@Temperature 120 °C
26800 psi

@Temperature 248 °F
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 185 MPa

@Temperature 60.0 °C
26800 psi

@Temperature 140 °F
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..
Tensile Strength at Break 185 MPa

@Temperature 23.0 °C
26800 psi

@Temperature 73.4 °F
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Tensile Strength at Break 185 MPa

@Temperature 23.0 °C
26800 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66  (Unverified Data**)
Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers
Tensile Strength at Break 185 MPa

@Temperature 23.0 °C
26800 psi

@Temperature 73.4 °F
ASTM D638
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige ..
Tensile Strength at Break 185 MPa

@Temperature 23.0 °C
26800 psi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..