Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -40.0 °C |
9.04 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1A |
DuPont Performance Polymers Hytrel® 6359FG NC010 TPC-ET
(Unverified Data**) Hytrel® 6359FG is a medium modulus Hytrel® grade with nominal durometer hardness of 63D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing t.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Europe-Africa-Middle East) Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors.This data was supplied b.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) Zytel® EFE7374 is a 40% fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for injection molding. It has an improved impact resistance and excellent surface appearance and gloss.I.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1A |
Ineos ABS Lustran® ABS 440 Injection Molding Grade Lustran® ABS 440 has medium impact strength and is injection molding grade. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 80 |
LG Chemical XR-472 ABS, High Heat Resistance, High Gloss Information Provided by LG Chem |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1A |
Lanxess Durethan® DP BKV 35 XF 901510 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
Styrolution Novodur® E401 ABS Novodur E401 is a high impact extrusion grade with good surface appearanceInformation provided by Styrolution |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styrolution Terluran® HH-106 Q109 Colored ABS Description: Injection-molding grade with high resistance to heat deformation and impact, with improved surface quality suitable for automotive applications.Information provided by STYROLUTION, whic.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styron Magnumâ„¢ 3453 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3453 ABS is a general purpose injection molding resin suitable for a wide range of applications.Information provided by DowThis product line was spun off from Dow Chemical to Styron in .. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 180/A |
Styron Magnumâ„¢ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ MED ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass (continuous process) ABS technology of Styron ensures an ABS resin that .. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Polyram PlusTek PA7800G33 Nylon 6.6 for Injection Molding, 33% Glass Fiber Reinforced, Heat Stabilized, Impact Modified 33% Glass fiber reinforced, heat stabilized, impact modified Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Polyram PlusTek PB302G50BK39P Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized 50% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by W.R.C. Potable Water and NSF/ANSI 61 International.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Polyram PlusTek PB302G50BK39D Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized 50% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by W.R.C. Potable Water and NSF/ANSI 61 International.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -40.0 °C |
9.04 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**) Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -40.0 °C |
9.04 ft-lb/in² @Temperature -40.0 °F |
Edgew 80x10x4; ISO 180/1A |
Eurostar Staramide BG6ST43 PA6, 30% Glass Fiber Filled, Impact Modified, Injection Molded BG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NB40 GR40 NL PA 6 40% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, Conditioned Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, Conditioned Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, Conditioned Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, Conditioned Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 0.000 °C |
9.04 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Europe-Africa-Middle East) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Izod Impact, Notched (ISO) | 19.0 kJ/m² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Verton PV007SV_WH8D537 PA 6 Preliminary data for 35% long fiber single pellet color filled PA6This data was supplied by SABIC-IP for the Americas region. |