Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unreinforced Polyamide 66Zytel EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
1.14 g/cc
0.0412 lb/in³
DAM; ISO 1183
Water Absorption 8.5 %

@Thickness 2.00 mm
8.5 %

@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 2.80 %

@Thickness 2.00 mm
2.80 %

@Thickness 0.0787 in
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.015 cm/cm
0.015 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.015 cm/cm
0.015 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 59.0 MPa
8560 psi
50%RH; ISO 527-1/-2
84.0 MPa
12200 psi
DAM; ISO 527-1/-2
Elongation at Break 18 %
18 %
DAM; Nominal; ISO 527-1/-2
>= 50 %
>= 50 %
50%RH; Nominal; ISO 527-1/-2
Elongation at Yield 4.5 %
4.5 %
DAM; ISO 527-1/-2
25 %
25 %
50%RH; ISO 527-1/-2
Tensile Modulus 1.50 GPa
218 ksi
50%RH; ISO 527-1/-2
3.00 GPa
435 ksi
DAM; ISO 527-1/-2
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
DAM; ISO 180/1A
10.0 kJ/m²
4.76 ft-lb/in²
50%RH; ISO 180/1A
Charpy Impact Unnotched NB
NB
DAM; ISO 179/1eU
NB
NB
50%RH; ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
DAM; ISO 179/1eA
1.20 J/cm²
5.71 ft-lb/in²
50%RH; ISO 179/1eA
Thermal Properties Metric English Comments
Specific Heat Capacity 2.79 J/g-°C
0.667 BTU/lb-°F
Thermal Conductivity 0.140 W/m-K
0.972 BTU-in/hr-ft²-°F
of melt
Melting Point 263 °C
505 °F
DAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
DAM; ISO 75-1/-2
Vicat Softening Point 257 °C
495 °F
DAM; 50°C/h 50N; ISO 306
Flammability, UL94 V-2

@Thickness 1.50 mm
V-2

@Thickness 0.0591 in
DAM; IEC 60695-11-10
V-2

@Thickness 0.700 mm
V-2

@Thickness 0.0276 in
DAM; IEC 60695-11-10
Oxygen Index 24 %
24 %
DAM; ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DAM; IEC 60093
Dielectric Strength 27.0 kV/mm
686 kV/in
DAM; IEC 60243-1
Dissipation Factor 0.010

@Frequency 100 Hz
0.010

@Frequency 100 Hz
DAM; IEC 60250
0.010

@Frequency 1.00e+6 Hz
0.010

@Frequency 1.00e+6 Hz
DAM; IEC 60250
Comparative Tracking Index 600 V
600 V
DAM; IEC 60112
Descriptive Properties Value Comments
Additives Lubricants
Release agent
Delivery Form Pellets
Part Marking Code >PA66<
ISO 11469
Processing Injection Moulding
Regional Availability Europe
Near East/Africa
Resin Identification PA66