Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | <= 0.950 g/cc | <= 0.0343 lb/in³ | ISO 1183 |
Murtfeldt Material ”S”® 1000 RB Polyethylene, High Friction An elastomer in Material ”S”® 1000 RB gives it high impact resistance and skid resistance.Special Properties:• High coefficient of friction• Good wear and abrasion resistanceInformation provide.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Orbilan RubberLen® R55 HMW-PE, dark blue ORBILAN RUBBERLEN® is a two-layered laminated panel made from Thermoplastic Elastomer (TPE) and low-pressure Polyethylene of High Molecular Weight (HMW-PE). RUBBERLEN® distinguishes itself by very.. |
|||
Density | 0.950 - 0.954 g/cc | 0.0343 - 0.0345 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6252J (526F2) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | TPE-0105 (ASTM D792) |
Advanced Elastomer Systems Trefsin® 3201-75 W305 Thermoplastic Rubber
(discontinued **) A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9404 HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: medium molecular weight distributions, wide range of processing conditions, low parison sag, good stress crack resistance. Federal specification LP390C .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® 9506H High Performance Series HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: superior physical properties, medium molecular weight distribution, wide range of processing conditions, low parison sag, excellent stress crack resistan.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Total Lacqtene® 2003 PBK 41 HDPE pipe, sheet
(discontinued **) LACQTENE® 2003 PBK 41 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2003 PBK 41 is a black compound especially developed for i.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | |
LyondellBasell Lupolen® 5021 D HDPE, Blow Molding Grade Easy flow, blow molding grade for small containers (up to 5 l), bottles for surface-active substances, household chemicals, laundry and dishwashing detergents, sanitary cleaners, cosmetics and pharm.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5005 1000 Micron EVA Powder Description: ICOFLO 510-5005 is an EVA powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in masterbatch (inste.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D1505 |
ICO Polymers ICOTEXâ„¢ 520-5005 1000 Micron EVA Powder Description: ICOTEX 520-5005 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: very high melt flow, fast melting, great .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Lushan EV1050G1 EVA Film for Encapsulating Solar modules, Ultra Fast Cure EVA film for encapsulating solar modules Lushan EV1050G1 is mainly used for PV module encapsulation. It’s based on an ethylene vinyle acetate (EVA) copolymer and supplemented by special Chemica.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
MTM Plastics Purpolen® PE Polyethylene Regrind Purpolen® is a sorted regrind material suited to the production of demanding end user products. Extrusion and injection molding grades are available in many colors. The basis of our Purpolen® .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
Stellarchem SV-B70E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Elvax® 3169Z Ethylene Vinyl Acetate DuPont™ Elvax® 3169Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3.. |
|||
Density | 0.950 g/cc @Temperature 23.0 °C |
0.0343 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group LOTRYL® 29 MA 03 Copolymer Ethylene - Methyl Acrylate LOTRYL® 29 MA 03 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 29 MA 03 is a polyme.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM-D1505 / ASTM-D792 |
Braskem Evateno® HM 2528 EVA Hot Melt Copolymer Evateno® HM 2528 is a copolymer of Ethylene-Vinyl Acetate (EVA) with high vinyl-acetate content, low molecular weight, and good compatibility with other thermoplastic and elastomeric resins, and it.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | |
3M Scotch-Weld™ AC68 Instant Adhesive Debonder 3M™ Scotch-Weld™ Instant Adhesive Debonder AC68 attacks and dissolves cured instant adhesives. It is formulated to have a relatively low evaporation rate and can be used to debond misaligned parts.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | |
Arkema Group Evatane® 1003 VL 4C Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 180 at 200 µ for greenhouse coverage.ISO data provided by the .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 1183 |
Barlog Plastics KEBAFLEX E 50.1 TPE-V, Shore A50 TPE-VInformation provided by BARLOG plastics GmbH. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | TPE-0105 (ASTM D792) |
Advanced Elastomer Systems Santoprene® 283-40 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Surlyn® 1707 Sodium Ionomer Surlyn® 1707 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t.. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
DuPont Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating 22.5 wt% Vinyl Acetate.Elvax® 3200-2 is an extrudable, wax-modified, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ASTM D792 |
Buckeye Polymers BP RPP 1010 T Polypropylene, 10% Mineral Filled This Talc-filled product exhibits excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistance, and resis.. |
|||
Density | 0.950 - 1.01 g/cc | 0.0343 - 0.0365 lb/in³ | Average value: 0.967 g/cc Grade Count:14 |
Overview of materials for Polypropylene with 10% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Density | 0.950 g/cc | 0.0343 lb/in³ | ISO 2781 |
KKPC KOSYN KTR 602 Thermoplastic Elastomer (TPE) Thermoplastic Elastomer (TPE)Characteristics: KOSYN KTR101 is linear block copolymer made by solution polymerization which polymerizes butadiene and styrene in organic solvent. It is thermoplastics .. |
|||
Density | 0.950 - 1.25 g/cc | 0.0343 - 0.0452 lb/in³ | Average value: 1.16 g/cc Grade Count:11 |
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum and .. |