Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.50 GPa | 218 ksi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PH 91 SD Polypropylene Modified homopolymer PP for injection molding. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol. s r.o. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PQ 82 N Polypropylene with improved impact strength PP impact modified. General application in all industry branches. Delivered in natural mode and in the full RAL color scale. For injection molding.Information Provided by Plastcom spol. s r.o. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | |
Plastcom SLOVALEN PC 63 T 15 PP reinforced with 15% mineral filler Features: Modified PP for injection moulding with the content of 15% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. Application in all automotive interior industry.D.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | |
Plastcom SLOVALEN PC 91 C 20 PP, 20% mineral filling FeaturesModified copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C depending on th.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO 527-1/-2 |
DSM Akulon® S223-E Nylon 66 (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-9524 20% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-9524 is a 20% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9524 is dev.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP HX03409C PA11 LNP* THERMOCOMP* HX03409C is a compound based on Nylon 11 resin containing Proprietary Filler(s). Added features of this material include: Clean Compound System, High Specific Gravity. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | 1mm/min; ISO 527-2 |
Borealis HF700SA Polypropylene HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.Infor.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | At 1 mm/min; ISO 527-2 |
Borealis Xmod™ BE677AI High Crystalline Polypropylene Copolymer Xmod BE677AI is a UV-stabilized HCPP intended for injection molding of automotive interior and appliance parts. Xmod BE677AI has an excellent balance between impact strength and stiffness as well .. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-530KF15 A5M Polymer Alloy Main Characteristics: High elongation; High impact strength; Stress resistantApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInformation provided by Zed.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ASTM D638 |
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin ISOPLAST® 101 is an engineering thermoplastic polyurethane resin.Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product li.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | cond; ISO 527-1/-2 |
DSM Novamid® 1010N2 1ES NAT PA6 FR(30) Injection Molding, Flame Retardant (Halogen free) |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | In Plane Direction |
Cymat A35620SC 040SS Stabilized Aluminum Foam Description: Cymat A35620SC 040SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.4 g/cm3. The mechanical properties of SAF make it .. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4155 black 9992 PA612-I Information provided by EMS Grivory |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO527-2/1 |
ExxonMobil PP1063L1 Polypropylene Homopolymer Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other .. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO527-2 |
ExxonMobil PPU0180F Polypropylene Homopolymer Product Description: An unstabilized homopolymer granular resin designed for automotive and compounding applications.Availability: Europe Processing Method: CompoundingInformation provided by Exxon.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO 527-2 |
Domo 1101P Polypropylene Homopolymer Information provided by Domo. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO 527-2 |
Domo 1104K Polypropylene Homopolymer Information provided by Domo. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high producti.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® RS LC1201 BK040A Nylon 1010
(Unverified Data**) Toughened Renewably Sourced Medium Viscosity Polyamide 1010 Developed for Extrusion Zytel RS LC1201 BK040A is a renewably sourced polyamide 1010 resin containing a minimum of 85% renewably sourced i.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ISO 527 |
Eurotec® Tecomid® NA40 NL IH PA 6.6 impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | ASTM D638 |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (7 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | |
BASF Gusspolyamid® Nylon 6 (At 50% RH) Processed by anionic polymerization of caprolactam in the presence of a catalyst and activator. Uses include semi-finished products and containers (e.g. heating oil tanks).Data was collected by ISO.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | |
BASF Novolen® 1101 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.50 GPa @Temperature 120 °C |
218 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Conditioned) Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | STN EN ISO 527-2 |
Plastcom SLOVALEN PH 91 N Polypropylene Homopolymer FeaturesModified homopolymer PP for injection moulding. General use in all industry branches - packing material, garden flower-pots, toys, furniture industry, hinges, fasteners, clamps, office chai.. |
|||
Tensile Modulus | 1.50 GPa | 218 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |