LyondellBasell Adsylâ„¢ 5C37F Thermoplastic Olefin Resin

Category Polymer , Thermoplastic
Manufacturer LyondellBasell
Trade Name Adsyl™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Adsylâ„¢ 5C37F Thermoplastic Olefin Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Primary Processing Method: Film extrusionKey Features: thermoplastic olefin resins for film extrusion, good clarity and gloss, good moisture barrier properties, very low seal initiation temperature, FDA acceptableApplications: food and non-food packaging, lamination filmsMeets FDA requirements in 21 CFR 177.1520 for all food contact, excluding cooking applications.Description: Adsyl 5C37F thermoplastic olefin resin are designed for film extrusion applications. It is formulated with slip and antilock. This resin is based on materials produced by Montell's proprietary Catalloy process. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for resins in rubber articles for repeated use applications. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 5.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 0.650 GPa
94.3 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.870 J/cm
1.63 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 63.0 °C
145 °F
ASTM D648