EMS-Grivory Grivory® BGM-30 X PA6-(GF+MD)30

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® BGM-30 X PA6-(GF+MD)30.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon BGM-30 X is a heat stabilized PA 6 injection molding grade with a 30 % reinforcement combination (mineral and glass fiber). Grilon BGM-30 X has the following important properties: High stiffnessLow warpageGood surface finish Grilon BGM-30 X is used typically for large area parts with low warpage such as radiator grilles or engine covers.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Water Absorption 8.0 %
8.0 %
ISO 62
Moisture Absorption 2.50 %
2.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 90.0 MPa
13100 psi
conditioned; ISO 2039-1
205 MPa
29700 psi
dry; ISO 2039-1
Tensile Strength at Break 45.0 MPa
6530 psi
conditioned; ISO 527-1/-2
105 MPa
15200 psi
dry; ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
dry; ISO 527-1/-2
15 %
15 %
conditioned; ISO 527-1/-2
Tensile Modulus 2.30 GPa
334 ksi
conditioned; ISO 527-1/-2
6.50 GPa
943 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
dry; ISO 179/1eU
6.00 J/cm²
28.6 ft-lb/in²
conditioned; ISO 179/1eU
3.50 J/cm²

@Temperature 30.0 °C
16.7 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
4.00 J/cm²

@Temperature 30.0 °C
19.0 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
dry; ISO 179/1eA
1.00 J/cm²
4.76 ft-lb/in²
conditioned; ISO 179/1eA
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 35.0 µm/m-°C
19.4 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
38.9 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long term; EMS
180 °C
356 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 175 °C
347 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 30.0 kV/mm
762 kV/in
conditioned; IEC 60243-1
34.0 kV/mm
864 kV/in
dry; IEC 60243-1
Comparative Tracking Index 500 V
500 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Cooling and climate control
Form Granules
Processing Injection Molding
Copyright © lookpolymers.com All Rights Reserved