Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75 |
Nilit FRIANYL A63 SG15 Nylon 6.6 for injection molding, 15% mineral filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75 |
Nilit FRIANYL B63 HS-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Unannealed; ASTM D648 |
PolyOne Edgetek® NL-10GF/000 BLACK Polyamide 612 (Nylon 612) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANMID 6 B12^ Q40 Nylon 6, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 103FHS BKB038 Nylon 66
(Unverified Data**) Zytel® 103FHS BKB038 is a heat stabilized, lubricated, PA 66 resin for fast cycling.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 - 252 °C | 392 - 485 °F | Average value: 235 °C Grade Count:10 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75-1/-2 |
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, DAM Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by G.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C @Thickness 6.40 mm |
392 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical Lupox® SG3250M PBT+PET+MF25% Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DIN 53461; ASTM D648 |
Kolon KOPA® KN163G30 G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | |
LATI Latiohm 88/10-06 CNT PEEK Semiconductive/dissipative product based on Polyetheretherketone (PEEK). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C @Thickness 3.20 mm |
392 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA6.12 LNP LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics ULTEM 9011 PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Ultem LTX300A PEI Copolymer (Europe-Africa-Middle East) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C @Thickness 3.20 mm |
392 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Stat-kon EE008E PEI LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas r.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 (Asia Pacific) LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C @Thickness 3.20 mm |
392 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C @Thickness 3.20 mm |
392 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 (Asia Pacific) NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6600 PA-66-HWL UL-Licensed Nylon 66, Flame Protection Grade V-2, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6600 PA-66-HWV0CP UL-Licensed Nylon 66, Flame Protection, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL BKB080 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75-1/-2 |
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Dry) Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
Eurostar Staramide BG3ST42 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG3ST42 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ASTM D648 |
Ashley Polymers Ashlene® 524 Nylon 66 A general purpose toughened Nylon 66.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75-2 |
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75-2 |
BASF Ultradur® S 4090 GM13 5/15% Glass/Mineral Filled PBT Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber and 15% mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventila.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics ULTEM 1000EF PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS. US FDA and EU Food Contact compliant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Unannealed; ISO 75-2/B |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |