Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 263 °C | 505 °F | DAM; ASTM D3418 |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) Zytel® 70G30HSL BK039B is a 30% glass reinforced, heat stabilized, black nylon 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® E41HSB NC010 Nylon 66
(Unverified Data**) Zytel® E41HSB is an unreinforced, high viscosity, heat stabilized polyamide 66 for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66
(Unverified Data**) Zytel® LM70G35HSLX is a 35% glass fiber reinforced, heat stabilized, lubricated polyamide 66 for injection molding. It is well suited for laser marking.Information provided by DuPont Performance Po.. |
|||
Melting Point | 263 °C | 505 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® AKV 30 HR H2.0 900116 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance |
|||
Melting Point | 263 °C | 505 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66 PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod.. |
|||
Melting Point | 263 °C | 505 °F | ISO 3146-C |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH0 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 246M PA66, DRY Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 50H1 PA66, DRY Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, DRY Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used.. |
|||
Melting Point | 263 °C | 505 °F | ISO 3146-C |
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH0 Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 216 S40 PA66, 40% glass spheres, DRY Description: Polyamide 66, reinforced with 40% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 216 S40 is used in all sectors of industry, offering a.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 216 V30 Natural FA PA66, 30% glass fiber, DRY Description: Polyamide PA66, reinforced with 30% of glass fiber and modified for enhanced injection molding.Available in: Europe Product Applications: This material offers an excellent combination b.. |
|||
Melting Point | <= 263 °C | <= 505 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LLDPE LL 3402.48 Blown Linear Low Density Polyethylene Resin Product Description: LL 3402.48 is a hexane medium density polyethylene blown film grade for applications requiring high stiffness. It can also be used in cast films. Films produced from the resin e.. |
|||
Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® E53 NC010 Nylon 66 Unreinforced High Viscosity Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66
(Unverified Data**) Unreinforced Toughened Polyamide 66 with Developed for Food Contact Applications Zytel FG408L NC010 is a general purpose lubricated impact modified polyamide 66 resin with superior toughness for inj.. |
|||
Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® FGFE5171 NC010C Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66 with Developed for Food Contact ApplicationsZytel FGFE5171 NC010C is a 33% glass filled nylon 66 resin. It has been developed for consideration into applications su.. |
|||
Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 BK010 is a 30% mineral reinforced flame retardant black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® ST800HSL BK152 Nylon 66
(Unverified Data**) Super Toughened Heat Stabilized Polyamide 66 Zytel ST800HSL BK152 is a heat stabilized Super Tough black polyamide 66 resin. It offers outstanding impact resistance high productivity and laser marka.. |
|||
Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Minlon® FE6190 BK086 Nylon 66 Minlon® FE6190 BK086 is a 36% mineral/glass reinforced, heat stabilized, black polyamide resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melting Point | 263 °C | 505 °F | ASTM D789 |
Adell AL-18 Nylon 66, 40% Glass Reinforced; Mineral Filled Data provided by Adell Plastics, Inc. |
|||
Melting Point | 263 °C | 505 °F | ASTM D789 |
Adell AR-18 Nylon 66, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® FGFE5171 NC010C Nylon 66
(Unverified Data**) Zytel® FGFE5171 NC010C is a 33% glass filled nylon 66 resin. It has been developed for consideration into applications such as parts for the food industry.Information provided by DuPont Performance.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. T.. |
|||
Melting Point | 263 °C | 505 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® BM70G15HSLR BK537 Nylon 66 Zytel® BM70G15HSLR BK537 is a 15% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Performance Polymers |
|||
Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® E41HSB NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E41HSB is an unreinforced high viscosity heat stabilized polyamide 66 for injection molding and extrusion.Information provided by DuPon.. |
|||
Melting Point | 263 °C | 505 °F | ISO 11357 |
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |