Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Clariant Renol 6608 HSL Nylon 66, High Impact Modified, Heat Stabilized, Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized , Nylon 66, Impact Grade
Manufacturer Clariant
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol 6608 HSL Nylon 66, High Impact Modified, Heat Stabilized, Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.014 - 0.019 cm/cm
0.014 - 0.019 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Elongation at Yield 50 %
50 %
ASTM D638
Flexural Yield Strength 55.2 MPa
8000 psi
ASTM D790
Flexural Modulus 1.59 GPa
230 ksi
ASTM D790
Izod Impact, Notched 8.28 J/cm

@Temperature 22.8 °C
15.5 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 157 °C
315 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.8 °C
145 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 266 - 288 °C
510 - 550 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm
Copyright © lookpolymers.com All Rights Reserved