Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 266 - 293 °C | 511 - 559 °F | |
PolyOne Gravi-Tech™ GRV-NY-035-SS-GF-BLK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc.. |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release Polycarbonate, General Purpose, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Melt Temperature | 266 - 282 °C | 511 - 540 °F | |
PolyOne Edgetek® TR2-30GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Melt Temperature | 266 - 282 °C | 511 - 540 °F | |
PolyOne Edgetek® X TR2-20TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Melt Temperature | 266 - 288 °C | 511 - 550 °F | |
Eastman Eastalloy DA510 Polymer
(discontinued **) Eastalloy Polymer DA510 is a clear copolyester/polycarbonate alloy. This product has good physical properties. These include good impact strength, chemical resistance, heat resistance, dimensional s.. |
|||
Melt Temperature | 266 - 288 °C | 511 - 550 °F | |
Eastman Eastalloy MA510 Polymer
(discontinued **) Eastalloy MA510 Polymer is a clear copolyester/polycarbonate alloy. It affords the consumer excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhan.. |
|||
Melt Temperature | 266 - 293 °C | 510 - 560 °F | |
Polymer Resources PC-UV4 Polycarbonate, UV-stabilized, Easy Flow Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
Ravago Manufacturing Americas Hylex® P1325L Polycarbonate, UV Stabilized, High Flow, Mold Release Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax BFM30-EL03N1 Nylon 6 30% Mineral Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax BFM30-EL03N1 Nylon 6 30% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax BFM40-DL04N1 Nylon 6 40% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG35-R113N1 Nylon 6 36% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG45-PN11N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
MTI ThermoStran® PA66-30C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Melt Temperature | 266 - 277 °C | 510 - 530 °F | |
Wellman Wellamid® FR22F-N Flame Retardant Nylon 66, Lubricated Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous.. |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol 6601FR Nylon 66, Flame Retardant Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol 6602-L Nylon 66, Internally Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol 6608-L Nylon 66, High Impact Modified, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol 6622-L Nylon 66, Glass Fiber Filled, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 288 °C | 510 - 550 °F | |
Clariant Renol PA111BK S&P Nylon 66, General Purpose Data provided by Clariant Masterbatches |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG30-QN11N1 Nylon 6 30% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG30-SN31N1 Nylon 6 30% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG33-RN13N1 Nylon 6 33% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 266 - 280 °C | 511 - 536 °F | ISO 294 |
Gromax CFG45-RN13N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |