Processing Properties Metric English Comments
Injection Pressure 2.76 - 8.27 MPa
400 - 1200 psi
RheTech Products FRP256-00 Polypropylene Copolymer, Flame Retardant, Natural
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant 612-01 HSL Black Nylon 612, Heat Stabilized
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant ABS4500 ABS, High Impact
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant PA123G20 Nylon 66, 20% Glass Fiber, Impact Modified, Heat Stabilized
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol 6001 M2 Nylon 6, Molybdenum Disulfide Lubricated
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol 60G13HSP Black Nylon 6, 13% Glass Fiber Reinforced, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol 612G20-L Nylon 612, 20% Glass Fiber Reinforced, Lubricated
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol BR2029 Nylon 66, General Purpose, Black
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PA113G13X050 Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Improved Ductility
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PA11BK FDA Nylon 66, General Purpose, FDA, Black
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PA211 Nylon 6, General Purpose
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PA211G13 Nylon 6, 13% Glass Fiber
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PA213 Nylon 6, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PA213G30 Nylon 6, 30% Glass Fiber, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PA213G36S Nylon 6, 36% Glass Fiber, Heat Stabilized, Silicone Lubricated
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PA233G13 Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Toughened
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PA2SP0007HW Nylon 6, Heavyweight Compound
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PA2SP0010HW Nylon 6, Heavyweight Compound
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PA2SP0011HW Nylon 6, Heavyweight Compound
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PA2SP0017 Nylon 6, Impact Modified
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PA2SP0022 Nylon 6, Impact and Flow Modified, ESD Protection, Black
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PBT1700 Polybutylene Terephthalate, Flame Retardant
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PCSP0007 Polycarbonate/Polyester Alloy
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PCSP0016BL-201 Polycarbonate/Polyester Alloy
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PPSP0005 Polypropylene Homopolymer, Glass Fiber and Mica Reinforced, Chemically Coupled
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol PPSS0007 Polyphenylene Sulfide, Glass Fiber and Mineral Filled
Data provided by Clariant Masterbatches
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
Clariant Renol TPU2072A Polyurethane Elastomer, Ether Based
Data provided by Clariant Masterbatches
Copyright © lookpolymers.com All Rights Reserved