Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 55.2 MPa | 8010 psi | ASTM D790 |
PolyOne Maxxam™ STFPP.1220 BK-L Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Yield Strength | 55.2 - 200 MPa | 8010 - 29000 psi | Average value: 112 MPa Grade Count:68 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Techmer ES Elastoblend® PBT E IM SL3 Availability: North AmericaForms: PelletsAdditive: Impact Modifier and Silicone LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 55.2 MPa | 8010 psi | |
Spartech Centrex® R83/21 ABS Weather Resistant Sheet Data provided by the manufacturer. |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Spartech Royalite R21 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Spartech Royalite R59 ABS/PVC Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Spartech SP-9030 Economy ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Techmer ES HiFill® PP GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Westlake Plastics Kynar® 740 PVDF Homopolymer Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab.. |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Devcon Brushable Ceramic - Red, Blue Epoxy Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,.. |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Entec Hylac® EX18 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Devcon Brushable Ceramic - White Epoxy Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,.. |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Devcon Sprayable Ceramic™ Epoxy Precision Repair EpoxyComments: A sprayable ceramic-reinforced composite that can be sprayed in a manner similar to high-solid paints. Ideal for protecting pumps, paper machines, stacks, pump pads,.. |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Clariant 612-01 HSL Black Nylon 612, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Clariant Renol 612-01L Nylon 612, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Clariant Renol PA1SP0004 Nylon 66, High Impact Modified, ESD Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Clariant Renol 6608 HSL Nylon 66, High Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Clariant Renol 6608-L Nylon 66, High Impact Modified, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Clariant Renol 6608-L UV Black Nylon 66, High Impact Modified, Lubricated, UV Stable Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 55.2 - 152 MPa | 8000 - 22000 psi | Average value: 79.7 MPa Grade Count:37 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Flexural Yield Strength | 55.2 - 193 MPa | 8000 - 28000 psi | Average value: 110 MPa Grade Count:28 |
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max.. |
|||
Flexural Yield Strength | 55.2 - 117 MPa | 8000 - 17000 psi | Average value: 90.3 MPa Grade Count:8 |
Overview of materials for Acrylic, UV Stabilized, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Yield Strength | 55.2 - 255 MPa | 8000 - 37000 psi | Average value: 165 MPa Grade Count:51 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |