Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 288 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 271 - 288 °C
520 - 550 °F
PlastiComp Complet® LGF40 - PA6 Nylon 6, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
Melt Temperature 260 - 288 °C
500 - 550 °F
Polymer Resources PC/TP-GP3-G30 PC/Polyester Alloy, 30% Glass Reinforced
Superior Chemical Resistance, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
Melt Temperature 260 - 288 °C
500 - 550 °F
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Melt Temperature 260 - 288 °C
500 - 550 °F
Air purge at equilibrium conditions
NOVA Chemicals Dylark® 378P30 Glass Reinforced Engineering Resin
Features: Ultra high modulus, High heat resistance, excellent adhesion to urethaneApplications: Instrument panel substrates, Brackets, Structural components
Melt Temperature 271 - 288 °C
520 - 550 °F
Ravago Manufacturing Americas Hylex® P1018LLT Polycarbonate
Information provided by Ravago.
Melt Temperature 249 - 288 °C
480 - 550 °F
RTP Company RTP 399 X 121668 B Polycarbonate (PC) Flame Retardant - Halogen Free - Wear Alloy - APWA (All Polymeric Wear Additive)
Melt Temperature 266 - 288 °C
511 - 550 °F
Eastman Eastalloy MA510 Polymer  (discontinued **)
Eastalloy MA510 Polymer is a clear copolyester/polycarbonate alloy. It affords the consumer excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhan..
Melt Temperature 249 - 288 °C
480 - 550 °F
Huntsman PE5080 Extrusion Coating Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings.FDA Notes: Conforms to FDA regulation 21 CFR..
Melt Temperature 249 - 288 °C
480 - 550 °F
Huntsman PE5082 Extrusion Coating Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings (sugar paper and laminations).FDA Notes: Con..
Melt Temperature 232 - 288 °C
450 - 550 °F
Molding
PolyOne Edgetek® AS-30CF/000 UV Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced  (discontinued
Description/Features:Carbon Fiber ReinforcedUV StabilizedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 204 - 288 °C
399 - 550 °F
Average value: 232 °C Grade Count:10
Overview of materials for Polypropylene, Fiber Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app..
Melt Temperature 271 - 288 °C
520 - 550 °F
Solvay Specialty Polymers Mindel® B-430 Polysulfone, Modified (PSU, Modified)  (discontinued **)
Mindel B-430 is a 30% glass reinforced thermoplastic with excellent dimensional stability, exceptional resistance to warp, good chemical resistance, and high stiffness. It was developed specifically..
Melt Temperature 271 - 288 °C
520 - 550 °F
Ravago Manufacturing Americas Hylon® N1025HLFR Nylon 6/6, 25% Fiberglass, Heat Stabilized, Lubricated, Flame retardant (Cond)
Information provided by Ravago.
Melt Temperature 260 - 288 °C
500 - 550 °F
PolyOne Gravi-Tech™ GRV-NP-069-BMX Nylon 12  (discontinued **)
Melt Temperature 246 - 288 °C
475 - 550 °F
Star Plastics PC/ABSQX7002 Molding Grade PC/ABS High Flow
Information provided by Star Plastics, Inc.
Melt Temperature 260 - 288 °C
500 - 550 °F
Westlake Hifor Xtreme SC74840 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74840 linear low density polyethylene is recommended for the core layer of cast stretch film. It provides excellent clarity and ultimate stretch values higher than the more c..
Melt Temperature 277 - 288 °C
530 - 550 °F
RTP Company RTP 1105 BLK Polyethylene Terephthalate (PET), Glass Fiber
Melt Temperature 224 - 288 °C
435 - 550 °F
RTP Company RTP 202 C FR Nylon 11 (PA); Glass Fiber - Flame Retardant - 50% Renewable Resource Content
Renewable Resource Content calculated based on % of total compound weight.
Melt Temperature 224 - 288 °C
435 - 550 °F
RTP Company RTP 203 C FR Nylon 11 (PA); Glass Fiber - Flame Retardant - 47% Renewable Resource Content
Renewable Resource Content calculated based on % of total compound weight.
Melt Temperature 224 - 288 °C
435 - 550 °F
RTP Company RTP 282 C Nylon 11 (PA), Carbon Fiber
Preliminary Data Sheet
Melt Temperature 224 - 288 °C
435 - 550 °F
RTP Company RTP 203 C Nylon 11 (PA); Glass Fiber - 79% Renewable Resource Content
Renewable Resource Content calculated based on % of total compound weight.
Melt Temperature 224 - 288 °C
435 - 550 °F
RTP Company RTP 203 C TFE 20 Nylon 11 (PA); Glass Fiber - PTFE Lubricated - 59% Renewable Resource Content
Renewable Resource Content calculated based on % of total compound weight.
Melt Temperature 266 - 288 °C
510 - 550 °F
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened
Data provided by Clariant Masterbatches
Melt Temperature 266 - 288 °C
510 - 550 °F
Clariant Renol PA101L Nylon 66, General Purpose, Lubricated
Data provided by Clariant Masterbatches
Melt Temperature 266 - 288 °C
510 - 550 °F
Clariant Renol PA101LRD-190 Nylon 66, General Purpose, Lubricated
Data provided by Clariant Masterbatches
Melt Temperature 266 - 288 °C
510 - 550 °F
Clariant Renol PA611D40 Nylon 612, Glass Fiber Reinforced, Molybdenum Disulfide Lubricated
Data provided by Clariant Masterbatches
Melt Temperature 266 - 288 °C
510 - 550 °F
Clariant Renol 6622-L Nylon 66, Glass Fiber Filled, Lubricated
Data provided by Clariant Masterbatches
Melt Temperature 266 - 288 °C
510 - 550 °F
Clariant Renol PA113G33 Nylon 66, 33% Glass Fiber, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Melt Temperature 260 - 288 °C
500 - 550 °F
Stock
PolyOne Lubri-Tech™ NI-30GF/15T Nylon 6/10 - 30% Glass Fiber Reinforced - 15% PTFE Lubricated  (discontinued *
Data provided by PolyOne.
Melt Temperature 210 - 288 °C
410 - 550 °F
RTP Company RTP 3382 Polyvinylidene Fluoride (PVDF), Carbon Fiber