Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Pro-faxâ„¢ RP320N Polypropylene Copolymer

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer LyondellBasell
Trade Name Pro-fax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-faxâ„¢ RP320N Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Pro-faxâ„¢ RP320N is a barefoot polypropylene random copolymer designed for cast film packaging applications. Cast film made with this resin has exceptional clarity and gloss, as well as improved cold temperature impact resistance and broader heat seal range compared to homopolymer polypropylene. Pro-faxâ„¢ RP320N resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Clear sheet, food packaging, bagsInformation provided by Basell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 81
81
ASTM D 785
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM D 638
Elongation at Yield 13 %
13 %
ASTM D 638
Flexural Modulus 0.924 GPa
134 ksi
1% Secant, 0.05 in/min; ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 81.1 °C
178 °F
Unannealed; ASTM D648