Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.59 GPa | 230 ksi | ASTM D790 |
Plaskolite Mustang PETG Sheet MUSTANG sheet signage material is continually processed using Eastman Tritan® copolyester, MUSTANG offers superior forming details, improved material distribution and shorter heating and cooling cy.. |
|||
Flexural Modulus | 1.59 GPa | 230 ksi | Tangent; ASTM D790 |
RheTech Products FT7013-720UV Thermoplastic Polyolefin, UV Stabilized, XTM Dark Sandstone Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | ASTM D790 |
PolyOne LubriOne™ PC-000/10T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 1.59 GPa | 230 ksi | ASTM D790 |
Nylene® 4121 (HS) Low Wear Nylon 6/6 Description: Nylene® 4121 (HS) is a high impact, low wear, 2% silicon oil reinforced nylon 6/6. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting compani.. |
|||
Flexural Modulus | 1.59 - 2.48 GPa | 230 - 360 ksi | Average value: 2.03 GPa Grade Count:22 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |
|||
Flexural Modulus | 1.59 GPa | 230 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH043EW Polypropylene, Homopolymer, Slit Film, LWCO, Cordage COPYLENE™ CH043EW is a medium flow polypropylene homopolymer resin suitable for general injection molding or extrusion applications. Applications: Raffia/tapes/strapping. Equivalent to Pro-fax® HL.. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | ASTM D790A |
Ineos H20Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Flexural Modulus | 1.59 GPa | 230 ksi | 1% Secant, 0.05 in/min; ASTM D790 |
LyondellBasell Moplen HP400L Polypropylene Homopolymer Description: All ingredients in HP400L meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Toys, containers, lids, medical applications, closure capsInformation provid.. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | 1% Secant; ASTM D790 |
Flint Hills P4G3Z-050 Homopolymer Polypropylene Homopolymer, FDA compliant.Features: Low water carryover.Applications: Extrusion: slit film and oriented fibers.Former Huntsman polypropylene products are now produced by Flint Hills Resources. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | 1% Secant at 0.05 in/min; ASTM D790 |
Ineos H03W-01 Polypropylene, Gas Phase Polymerized H03W-01 (formerly Fortilene® HG3253) belongs to the new generation of polypropylenes produced by gas phase polymerization. This nominal 4 melt flow index product is specifically designed for fib.. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ML004 PP LNP* LUBRICOMP* ML004 is a product based on Polypropylene containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Flexural Modulus | 1.59 GPa | 230 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM 511 HS L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUses: Low Temperature ApplicationsInformatio.. |
|||
Flexural Modulus | 1.59 GPa | 230 ksi | tangent; ASTM D790 |
Spartech PP7120 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | ASTM D790 |
UBE UBESTA® 3035LU1 Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Flexural Modulus | 1.59 GPa | 230 ksi | 2% Secant; ASTM D790B |
ExxonMobil HDPE HD 6909.19 High Density Polyethylene Copolymer Resin Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ.. |
|||
Flexural Modulus | 1.59 GPa | 231 ksi | ASTM D790 |
Engineered Plastics EPABS 19 ABS Extrusion Grade Pellets. GMP # 002. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Flexural Modulus | 1.59 GPa | 230 ksi | 1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A |
Dow H110-02N Polypropylene Resin DOW H110-02N is intended for use in extrusion and thermoforming processes. It is especially suited for applications where improved melt strength and clarity are desired.Information provided by DowD.. |
|||
Flexural Modulus | 1.59 GPa | 230 ksi | ASTM D790 |
Clariant Renol CAB1000 Cellulose Acetate Butyrate Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.59 GPa | 230 ksi | ASTM D790 |
Clariant Renol 6608-L Nylon 66, High Impact Modified, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.59 GPa | 230 ksi | ASTM D790 |
Clariant Renol 6608-L UV Black Nylon 66, High Impact Modified, Lubricated, UV Stable Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.59 GPa | 230 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem D115A Homopolymer Polypropylene Description: Multi Purpose, Good Color and Process StabilityApplications: Suggested Uses Include Housewares, Patio Furniture, ClosuresThis resin meets the requirements for olefin polymers as defined.. |
|||
Flexural Modulus | 1.59 GPa | 230 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem FT120WB2 Homopolymer Polypropylene Description: Superior Antistatic properties, excellent mold release.Applications: Suggested uses include closures, housewares.Process: Injection Molding.This resin meets the requirements for olefin .. |
|||
Flexural Modulus | 1.59 GPa | 230 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI2350C High Crystallinity Copolymer Polypropylene Description: Highly crystalline homopolymer phase, very high molecular weight ERP phase, very high flexural modulus, reduced emissions, reduced gels.Applications: Suggested uses include compounding... |
|||
Flexural Modulus | 1.59 - 2.07 GPa | 230 - 300 ksi | ASTM D790 |
Buckeye Polymers BP RPPC 2008 C BLK Polypropylene, Calcium Filled Product Information: Calcium Carbonate Filled PP Grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. Our BP RPP C series product line ranges fro.. |
|||
Flexural Modulus | 1.59 GPa | 230 ksi | ASTM D790 |
Americas Styrenics EA6740 High Impact Polystyrene Product CharacteristicsVery good printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsPackaging and one-time use it.. |