Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
Polymer Resources NY66-GP1-[color]H Nylon, General Purpose Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized General Purpose Nylon 66, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Mold Temperature | 76.7 - 93.3 °C | 170 - 200 °F | |
Ravago Manufacturing Americas Hylex® P1010LLT Polycarbonate Information provided by Ravago. |
|||
Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
Celanese Celanex® 4022 PBT, Specialty
(Unverified Data**) A white PBT resin typically used for applications requiring very opaque parts.PBT, opaque whiteInformation provided by Celanese |
|||
Mold Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
Northstar Polymers MGP-D50A High Performance Polyurethane Cast Elastomer System 50D This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires some load-bearing, slide abrasion, constant water contac.. |
|||
Mold Temperature | 48.9 - 93.3 °C | 120 - 200 °F | |
Ravago Manufacturing Americas Hylon® N1000TL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago |
|||
Mold Temperature | 54.4 - 93.3 °C | 130 - 200 °F | Average value: 73.9 °C Grade Count:24 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Mold Temperature | 60.0 - 93.3 °C | 140 - 200 °F | |
RTP Company RTP 281D TFE 15 Nylon 6/12 (PA 6/12) Carbon Fiber 10% - PTFE 15%
(discontinued Carbon Fiber 10% - PTFE 15%Comments:Carbon FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provi.. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 6 GB30 30% Glass Bead Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 6 GF33RN 33% Glass Bead Reinforced, Industrial Grade Nylon 6 Information provided by A. Schulman. |
|||
Mold Temperature | 60.0 - 93.3 °C | 140 - 200 °F | |
RTP Company RTP 200 D MS Nylon 6/12 (PA), Molybdenum Disulfide |
|||
Mold Temperature | 51.7 - 93.3 °C | 125 - 200 °F | |
RTP Company RTP 2309 A Rigid Thermoplastic Polyurethane (RTPU), Glass Fiber |
|||
Mold Temperature | 51.7 - 93.3 °C | 125 - 200 °F | |
RTP Company RTP 2382 A Rigid Thermoplastic Polyurethane (RTPU), Carbon Fiber |
|||
Mold Temperature | 51.7 - 93.3 °C | 125 - 200 °F | |
RTP Company RTP 2599 X 65037 FR A Polycarbonate/ABS Alloy (PC/ABS), Glass Fiber - PTFE Lubricated - Flame Retardant - UL94 V-0 |
|||
Mold Temperature | 48.9 - 93.3 °C | 120 - 200 °F | |
RTP Company PermaStat® 600 FR Acrylonitrile Butadiene Styrene (ABS), ESD Protection - Permanently Anti-static - Flame Retardant |
|||
Mold Temperature | 76.7 - 93.3 °C | 170 - 200 °F | |
Entec Hylex® P1310FR Polycarbonate Information provided by Ravago |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
Clariant Renol 6001 M2 Nylon 6, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
Clariant Renol PA113 Nylon 66, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
Clariant Renol PA133 Nylon 66, Highly Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
Engineered Polymer Solutions PBT VM 450, 20% Mineral Filled Plate-able. Natural and colors available. Injection molding grade. Uses: Automotive, appliancesInformation provided by Engineered Polymer Solutions. |
|||
Mold Temperature | 60.0 - 93.3 °C | 140 - 200 °F | |
RTP Company RTP 201D Nylon 6/12 (PA 6/12) Glass Fiber 10%
(discontinued **) Glass Fiber 10%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for .. |
|||
Mold Temperature | 60.0 - 93.3 °C | 140 - 200 °F | |
RTP Company RTP 283D TFE 15 Nylon 6/12 (PA 6/12) Carbon Fiber 20% - PTFE 15%
(discontinued Carbon Fiber 20% - PTFE 15%Comments:Carbon FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provi.. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
A. Schulman SCHULAMID® 66 GF30H 30% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
RTP Company RTP 1701 FR Modified Polyphenylene Oxide (PPO), Glass Fiber - Flame Retardant - Halogen Free |
|||
Mold Temperature | 54.4 - 93.3 °C | 130 - 200 °F | |
RTP Company RTP 299 A X 92682 D Nylon 6 (PA), High Gravity Compound - Easy Molding |
|||
Mold Temperature | 37.8 - 93.3 °C | 100 - 200 °F | |
RTP Company RTP 3405-1 Liquid Crystal Polymer (LCP), Glass Fiber |
|||
Mold Temperature | 65.6 - 93.3 °C | 150 - 200 °F | |
RTP Company RTP 3487-4 Liquid Crystal Polymer (LCP), Carbon Fiber |
|||
Mold Temperature | 37.8 - 93.3 °C | 100 - 200 °F | |
Celanese Vandar® 2100UV PBT, Impact Modified
(Unverified Data**) Vandar 2100UV is a polyester alloy designed to offer maximum impact strength at room and low temperatures. This unfilled compound is characterized by outstanding chemical resistance, dimensional sta.. |
|||
Mold Temperature | 54.4 - 93.3 °C | 130 - 200 °F | |
RTP Company RTP 206 A HS Nylon 6 (PA), Glass Fiber - Heat Stabilized |