Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis BL0521 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Borealis
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Borealis BL0521 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BL0521 is a high molecular weight (HMW), high density polyethylene. The main properties are: good impact resistance, high stiffness, very good stress crack resistance. Applications: cans and drums from 5 liters and upwards, and containers intended for transport of dangerous goods according to UN regulations.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ISO 1183
Environmental Stress Crack Resistance >= 300 hour
>= 300 hour
Antarox 10%; ASTM D1693-A
Melt Flow 2.5 g/10 min
<br>@Load 21.6 kg,<br> Temperature 190 °C
2.5 g/10 min
<br>@Load 47.6 lb,<br> Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ISO 868
Tensile Strength, Yield 26.0 MPa
3770 psi
50mm/min; ISO 527-2
Elongation at Yield 10 %
10 %
50mm/min; ISO 527-2
Tensile Modulus 1.10 GPa
160 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 3.00 J/cm²
<br>@Temperature -20.0 °C
14.3 ft-lb/in²
<br>@Temperature -4.00 °F
ISO 179/1eA
3.50 J/cm²
<br>@Temperature 23.0 °C
16.7 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ISO 75-2
Processing Properties Metric English Comments
Middle Barrel Temperature 190 - 220 °C
374 - 428 °F
Die Temperature 180 - 220 °C
356 - 428 °F
Melt Temperature 180 - 220 °C
356 - 428 °F
Copyright © lookpolymers.com All Rights Reserved