Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
SABIC M40053S High Density Polyethylene for Injection Molding Product Description: M40053S is a UV stabilized high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to pro.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ISO 1183 |
Total Finathene® 53140 HDPE, blow molding, sheet
(discontinued **) Finathene® 53140 is a high density polyethylene produced by the slurry loop low pressure polymerization process FINATHENE® 53140 has been especially developed for the manufacturing of blow molded .. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ISO 1183 |
Total Finathene® 56020 HDPE, blow molding, sheet
(discontinued **) FINATHENE® 56020 S is a very high molecular weight high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® 56020 S has been especially developed for t.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 767.MJ Blown Film Resin
(discontinued **) Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 767.MJ Cast and Compounding Film Resin
(discontinued **) Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D 792 |
Total Finathene® 5302 HDPE drain tile, corrugated pipe resin
(discontinued **) Applications: corrugated pipe, storm and sanitary sewers, drainage systemsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics produc.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® LH5320 Injection Molding HDPE
(discontinued **) CopolymerApplications: Housewares, bowls, food containers, toysFormolene LH5320 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Adm.. |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2712 HDPE Injection Molding Resin Features: Good stiffness and impact resistance, minimal warpage, good top loading capability, high surface gloss.Applications: Aerosol overcaps, food containers, frozen food containers, seedling tra.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | |
LyondellBasell Lupolen® 5231 HX HDPE, Impact Grade Medium flow, impact resistant, very stress-crack resistant grade for closures, bottles that contain carbonated liquids, storage and tote boxes, as well as engineering components.Data was collected b.. |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | |
LyondellBasell Lupolen® 5261 ZS HDPE, Blow Molding Grade Relatively high viscosity blow molding grade (similar to Lupolen 5261 Z), but more resistant to stress cracking) for rigid, stackable and highly shock resistant containers for packaging all types of.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LR732031 High Density Polyethylene ApplicationsPETROTHENE LR 7320-31 is a high density polyethylene resin that exhibits an excellent balance of stiffness and environmental stress crack resistance. This resin has outstanding extrusio.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LR734011 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LR734045 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Plexar® PX2246 Extrudable Tie-Layer Resin - Anhydride Modified HDPE General DescriptionPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resin.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® HD 5301 EA HDPE Blow Molding Applications:High performance blow molded containers typically of to 60 liters capacity for packaging aggressive productsRobust industrial and technical moldingsInformation provided by Interchim s.r.. |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | ISO 1183 |
Borealis Borstar® HE3476-LS Yellow Polyethylene Compound for The Coextrusion of Identifying Stripes On Black HD Pipe for Natural Gas Borstar HE3476-LS is a bimodal, cadmium free, high density polyethylene compound designed for coextrusion of blue identifying stripes. It is fully stabilized against thermal degradation and the die.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® FB 85 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® 9004 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® 9012 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 232, A 55600Characteristics: Good Flow, Good Impact Strength, Good Stiffness, Good ESCR, Good Shrinkage ResistanceApplications:Food Pails.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® AD2528 Adhesive Application Resin Escorene Ultra AD 2528 is a very high flow rate, 27.6% Vinyl Acetate, copolymer, which is useful in formulating hot melt adhesives.Availability: Latin America, North America and South America Additi.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ExxonMobil method |
ExxonMobil HDPE HD 6706.62 High Density Polyethylene Copolymer Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ExxonMobil method |
ExxonMobil HDPE HD 6719.62 High Density Polyethylene Copolymer Resin Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D4883 |
ExxonMobil HDPE HTA 002 High Density Polyethylene Resin Product Description: HTA 002 is a general purpose medium molecular weight HDPE grade, characterized by easy processability, especially in coextrusion and blending with other polyolefins. HTA 002 can.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D792 |
Entec Hypel® PEHD20/.953 HDPE Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | |
Dow DOWLEX™ IP-40 High Density Polyethylene DOWLEX® IP-40 resin is an improved processing high density resin designed to offer excellent processability and impact resistance required for food container applications. This resin is designed by.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® HHM 5202-02 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers .. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D4883 |
ExxonMobil HD 6706.62 Injection Molding Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Density | >= 0.952 g/cc | >= 0.0344 lb/in³ | UNI EN ISO 1183-1 |
Breplast Bretene TST High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Bapolene® 3252 Polyethylene, Injection Grade Narrow molecular weight distribution injection molding resin. This resin offers excellent impact strength, ESCR properties, and resistance to warpage. This product meets the Food and Drug Administ.. |
|||
Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Ineos J50-1000-181 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still water. This resin c.. |