Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.10 GPa | 160 ksi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PQ 81 T 15/1 Polypropylene reinforced with mineral filler, impact modified Modified PP for injection molding with the content of 15% mineral filler. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.o. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | |
Plastcom SLOVALEN PQ 81 T 15 PP, 15% mineral filling FeaturesModified PP for injection moulding with the content of 15% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | |
Plastcom SLOVAMID 6 LI PA6, improved strength FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | |
LyondellBasell Lupolen® 5231 HX HDPE, Impact Grade Medium flow, impact resistant, very stress-crack resistant grade for closures, bottles that contain carbonated liquids, storage and tote boxes, as well as engineering components.Data was collected b.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | |
LyondellBasell Lupolen® 5236 HX HDPE, Impact Grade Medium flow, impact resistant, high stress-crack resistant grade for closures for bottles that contain carbonated liquids. This product contains a slip agent.Data was collected by ISO methods and o.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ASTM D638 |
Ineos Styrenics Polystyrene 486N (NAFTA) High-impact grade of polystyrene with excellent ESCR.Information provided by BASF.Ineos Styrenics purchased this product line from BASF in 2005. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | |
LATI Latiohm 83-07 PD11 CNT PA12, Impact Modified Semiconductive/dissipative product based on Polyamide 12 (PA12), impact modified. Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ISO 527 |
Solvay Technyl® C 206 Nylon 6, EH50 Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 206 PA6, Conditioned Description: Unreinforced Polyamide PA6, standard for fast cycling, for injection molding.Available in: EuropeProduct Applications: TECHNYL® C 206 has fluidity and a good mould release, favored b.. |
|||
Tensile Modulus | 1.10 - 1.30 GPa | 160 - 189 ksi | MD; ISO 527-3 |
Borealis BorPURE™ RB501BF Polypropylene Copolymer BorPure™ RB501BF is a random copolymer. Applications: BorPure™ RB501BF has been developed especially for applications like: food packaging, over wrap film, label film, and shrink film. Additives.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 1mm/min; ISO 527-2 |
Borealis BS2541 High Density Polyethylene BS2541 is a high density polyethylene with very high ESCR This product is intended for blow molding. Applications: household and chemical containers such as detergents, cleaners, and motor oils, an.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | TD; ASTM D882-A |
Borealis FS1470 High Density Polyethylene FS1470 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1470 have high impact and tensile strength, and bala.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | |
Covestro Bayflex® 110-50 Polyurethane Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® FG 34 NL nat 6023 PA6 Product description: Grilon FG 34 NL natural 6023 is a modified, medium viscosity polyamide 6. Grilon FG 34 NL natural 6023 exhibits following improvements compared to a PA 6: Better gas barrier pro.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® FG 40 NL nat 6025 PA6 Product description: Grilon FG 40 NL natural 6025 is a modified, high viscosity polyamide 6. Compared to conventional polyamide 6 Grilon FG40 NL natural 6025 offers the following improvements:Better.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® FG 47 NL nat 6028 PA6 Product description: Grilon FG 47 NL natural 6028 is a modified, high viscosity Polyamide 6, which contains also slip and nucleating agents. Grilon FG 47 NL natural 6028 shows following improvements.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 G grey 9280 PA12 Product Description: Grilamid L 20 G grey 9280 is a medium viscosity, unreinforced, heat stabilized polyamide 12 for injection molding and cable sheathing. The main features of this product are: Low.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 G PA12 Product Description: Grilamid L 20 LG is a normal viscosity, heat stabilized polyamide 12 non-reinforced injection molding grade. This product has very good flow characteristics Low moisture absorpt.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20H FWA black 9225 PA12 Product Description Grilamid L 20 H FWA black 9225 is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA black 9225 is used for technical injection molded .. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ CNU 013 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with good UV resistance designed for automotive exterior applications. Availability: Africa & Middle East, Asia Pacific, Europe, South.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 H PA12 Product Description: Grilamid L 25 H is a high viscosity heat stabilized Polyamide 12 extrusion grade and is suitable for application requiring a long-term usage temperature of 100 - 120°C. The mai.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**) Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 Polyamide 6 - Natural Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechanical strength, rigidi.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 (2414) PA 6.6 Conditioned AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | |
BASF Novolen® 3248 RC Polypropylene Grade containing nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ASTM D638 |
Lubrizol Stat-Rite® SIS535 Static Control System Product Description: Stat-Rite® SIS535 is a static dissipative HIPS alloy. Stat-Rite SIS535 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, perma.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |