Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Europe-Africa-Middle East) CYCOLOY C1200 is a PC+ABS blend developed to serve extremely demanding applications in a variety of markets while maintaining good processing properties. The combination of superior heat resistance .. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYblend 45FS PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYblend 85 M10 PC/ABS-Blend Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYelast TPE 10012 R3 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 3.00 J/cm² @Thickness 102 mm, Temperature 23.0 °C |
14.3 ft-lb/in² @Thickness 4.00 in, Temperature 73.4 °F |
ISO 179 |
Premix Thermoplastics PRE-ELEC® PP 1398 Conductive Thermoplastic Compound PRE-ELEC® PP 1398 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANBLEND SS7 PC/ASA, UV-Resistant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature -20.0 °C |
14.3 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANTEC PC M75R Polycarbonate, Steam Resistant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
Qualchem Danamid FES-23 HUV Polyamide 6 Impact resistant, cold. Heat and UV stabilized, for long-lasting use at 120-130°C, protected against artificial light.Information provided by Qualchem Zrt. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature -20.0 °C |
14.3 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANTEC PC S75R Polycarbonate Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K230-HXG6 Nylon 6-30% Glass Reinforced (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-2120 17TOP BU UV-Stabilized 17% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-2120 17TOP BU is a black colored, 17% talc-filled, UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-2120 17TOP BU is developed for producing injection .. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-3302 Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-3302 is an elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-3302 is developed for produ.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature -20.0 °C |
14.3 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-8302 Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-8302 is an elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-8302 is developed for extru.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eA |
Ineos ABS Lustran® Ultra 4105 ABS Pellets (Polycarbonate-modified), Medium High Heat Grade Lustran® Ultra 4105 is medium high heat grade with superior impact resistance. It is PC-modified and has low emission. It is used for the production of molded plastic articles. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature -20.0 °C |
14.3 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis BL0521 High Density Polyethylene BL0521 is a high molecular weight (HMW), high density polyethylene. The main properties are: good impact resistance, high stiffness, very good stress crack resistance. Applications: cans and drums .. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis Daplen™ ED230HP Polypropylene TPO Compound Daplen™ ED230HP is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis Daplen™ EG250AI Polypropylene TPO Compound Daplen™ EG250AI is a 20% mineral reinforced impact modified polypropylene compound suitable for injection molding. This material has an excellent balance between impact strength and stiffness, giv.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-G6U (Cond.) 33% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-PG8 (Dry) 40% Glass Reinforced, Impact Modified Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature -40.0 °C |
14.3 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® FN718 BK230A Nylon 66
(Unverified Data**) Zytel® FN718 BK230A is a flexible, plasticizer free modified black polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
DIN ISO 179 |
BASF Elastollan R 3001 15% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, Conditioned Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX1482T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC Copolymer, enhanced UV stabilization. Transprarent and tinted colors. Higher mold release content than SLX1432T.This data was supplied by SABIC-IP for the Europe-Africa-Middle E.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 67R Nylon 66, Heat Stabilized, Conditioned Vydyne® 67R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67R resin offers high strength, .. |