Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 300 hour | 300 hour | Condition A (10% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® L63550U Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Formolene L63550 is fully heat and UV stabilized.Meets all requirements.. |
|||
Environmental Stress Crack Resistance | 300 hour | 300 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 8406 BK, 8406 GBK MDPE Rotational Molding Resin
(discontinued **) Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | 300 hour | 300 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 8406 UV8D, 8406G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | 300 - 600 hour | 300 - 600 hour | Average value: 500 hour Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Environmental Stress Crack Resistance | 300 hour | 300 hour | |
JPJ Technologies 700F HDPE Extrusion Information provided by JPJ Technologies |
|||
Environmental Stress Crack Resistance | 300 hour @Temperature 50.0 °C |
300 hour @Temperature 122 °F |
F50, 25% Igepal; ASTM D1693 |
SCG Chemicals EL-Leneâ„¢ H5840B High Density Polyethylene Blow Molding Key Characteristics:Excellent environmental stress cracking resistance (ESCR)Excellent appearanceOdorlessSafe for food contactGood printabilityRecommended Applications: Bottles for food, juice, sof.. |
|||
Environmental Stress Crack Resistance | >= 300 hour | >= 300 hour | Antarox 10%; ASTM D1693-A |
Borealis BL0521 High Density Polyethylene BL0521 is a high molecular weight (HMW), high density polyethylene. The main properties are: good impact resistance, high stiffness, very good stress crack resistance. Applications: cans and drums .. |
|||
Environmental Stress Crack Resistance | 300 hour | 300 hour | Antarox 10%, F50; ASTM D1693-A |
Borealis BL1481 High Density Polyethylene BL1481 is a semi high molecular weight polyethylene comprising an extra ordinary ESCR and very good chemical resistance This product is intended for blow molding. This grade is available in granular.. |