Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.10 GPa | 160 ksi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PQ 81 T 15/1 Polypropylene reinforced with mineral filler, impact modified Modified PP for injection molding with the content of 15% mineral filler. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.o. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ISO.527 DIN.53455 |
Omnia Plastica PP Polypropylene The mechanical features of PP are better than those of PE H.D. It withstands attack by alkali and acids and consequently it is widely used for components in the chemical industry when a moderate str.. |
|||
Tensile Modulus | >= 1.10 GPa | >= 160 ksi | 1 mm/min; ISO 527 |
MTM Plastics Dipolen® PP Recycled PP Dipolen® PP is a granulated polypropylene for use in either extrusion or injection molding. It can be supplied unmodified or treated with additives according to customer specifications. DipolenÂ.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 216 PA6, Conditioned Description: Unreinforced polyamide PA6, standard nucleation for fast cycling, for injection molding.Available in: Asia PacificProduct Applications: This grade has a high fluidity and good mould rel.. |
|||
Tensile Modulus | 1.10 - 1.35 GPa @Thickness 1.50 mm |
160 - 196 ksi @Thickness 0.0591 in |
1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 60512/0550 and 60512/0150 Polyvinylidene Fluoride (PVDF) Solef® 60512/0550 and Solef® 60512/0150 are PVDF grades compounded with PTFE for extrusion of anti-wear tapes.Features: CopolymerUses: TapeAdditional Properties: Crystallization Heat - ASTM D3.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON WS002I PBT (Asia Pacific) LNP* Stat-kon* WS002I is a compound based on Polybutylene Terephalate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP (Europe-Africa-Middle East) LNP* Stat-loy* M3000 is a compound based on Polypropylene resin. Added features of this material include: Antistat, High Impact. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ASTM D638 |
Lubrizol Stat-Rite® S-680 Static Control PETG Alloy Stat-Rite® S-680 is a static dissipative PETG alloy. Stat-Rite® M-680 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio.. |
|||
Tensile Modulus | 1.10 - 1.30 GPa | 160 - 189 ksi | MD; ISO 527-3 |
Borealis BorPURE™ RB501BF Polypropylene Copolymer BorPure™ RB501BF is a random copolymer. Applications: BorPure™ RB501BF has been developed especially for applications like: food packaging, over wrap film, label film, and shrink film. Additives.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 1mm/min; ISO 527-3 |
Borealis RE420MO Polypropylene Random Copolymer, Transparent RE420MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is intended for injection molding and stretch blow molding. and is designed .. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | At 1 mm/min; ISO 527-2 |
Borealis Borstar® HE3492-LS Yellow-Orange High Density Polyethylene for Natural Gas Pipes Borstar HE3492-LS is a yellow-orange, cadmium free, high density polyethylene compound classified as a MRS 10.0 material (PE100) produced with the advanced Borstar technology. It includes a combina.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ISO 527-1/-2 |
DSM Arnitel® EL740-H/A Injection Molding; Other Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BS/2 PA6 Product description: Grilon BS/2 is an unreinforced, nucleated standard PA6 injection molding grade with normal melt viscosity. Grilon BS/2 has the following important properties: Good flow behavior.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® FG 40 NL nat 6018 PA6 Information provided by EMS Grivory |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 G PA12 Product Description: Grilamid L 20 LG is a normal viscosity, heat stabilized polyamide 12 non-reinforced injection molding grade. This product has very good flow characteristics Low moisture absorpt.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20H FWA black 9225 PA12 Product Description Grilamid L 20 H FWA black 9225 is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA black 9225 is used for technical injection molded .. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 3926 black 9992 PA12 Product description: Grilamid XE 3926 black 9992 is a low viscosity extrusion type, based on Polyamide 12 (PA 12). The special features of Grilamid XE 3926 black 9992 are: Very good chemical resista.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ISO 527 |
Eurotec® Tecoform® PO20 NL IL POM, impact modified, natural Information provided by Eurotec® |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20H FWA nat PA12 Product Description: Grilamid L 20 H FWA natural is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA natural is used for technical injection molded parts.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 H PA12 Product Description: Grilamid L 25 H is a high viscosity heat stabilized Polyamide 12 extrusion grade and is suitable for application requiring a long-term usage temperature of 100 - 120°C. The mai.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ASTM D638 |
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness) AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MS Polyamide 6 - Natural Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.For uncolored parts produced by injection molding, contain including and demo.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | |
BASF Novolen® 3240 NC Polypropylene Grade containing nucleating agent for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ CNW 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior trim applications requiring low warpage.Availability: Africa & Middle East, Asia Pac.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | ASTM D638 |
Lubrizol Stat-Rite® SIS535 Static Control System Product Description: Stat-Rite® SIS535 is a static dissipative HIPS alloy. Stat-Rite SIS535 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, perma.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |
|||
Tensile Modulus | 1.10 GPa | 160 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific) LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |