Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
SABIC F00952 High Density Polyethylene for Blown Film Product Description: F00952 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Network Polymers NPP 50-1052 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® HB-W952-A HDPE Extrusion Resin Molded Plaque Properties. Features: High molecular weight, excellent ESCR, impact strength, high rigidity.Applications: large-part blow-molding, trash cans, drums, jerry cans, fuel tanks.Data provi.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Huntsman Rexell® H2110 Injection Molding LLDPE
(discontinued **) Linear-low high density injection molding.Features: Good toughness, ESCR.Applications: Industrial and consumer pails, general purpose molding.Information provided by Huntsman Corporation |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9035 HDPE Injection Molding Resin
(discontinued **) Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9650 HDPE Blown Film Resin
(discontinued **) Resin Type: Linear Polyethylene CopolymerCharacteristics: Copolymerization Enhances Film Toughness, Excellent Film Drawdown, Unique Molecular Architecture Gives Moisture Barrier Properties Typical o.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D4883 |
ExxonMobil HD 6761.17 Injection Molding Resin
(discontinued **) HD 6761 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a heavy-d.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 767.MJ Cast and Compounding Film Resin
(discontinued **) Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® LH5206 Injection Molding HDPE
(discontinued **) CopolymerApplications: Pails, lidsFormolene LH5206 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Administration as specified in 2.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | |
LyondellBasell Lupolen® 5231 HX HDPE, Impact Grade Medium flow, impact resistant, very stress-crack resistant grade for closures, bottles that contain carbonated liquids, storage and tote boxes, as well as engineering components.Data was collected b.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 150-1498 HDPE Rotational Molding Resin Description: ICORENE 150-1498 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. This product is.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Ineos J50-200-178 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the molding of screw caps dedicated to the packaging of carbonated beverages. This material m.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Ineos T50-200 HDPE Ineos T50-200 is a high density polyethylene copolymer of narrow molecular weight distribution. It is intended for injection molding applications which require high impact resistance and good envir.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) BL6 HM7255 High Density Polyethylene BL6 (HM 755) is a high density polyethylene with Butene-1 as a comonomer. It is a high molar mass material with very good impact strength, stiffness, and stress cracking resistance.Applications: la.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D792 |
IRPC Polimaxx Polene GA3750 High Density Polyethylene CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® HD 5211 EA HDPE Injection Molding Applications:Paint pailsBottle capsHouse waresToysInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® HD 5218 EA HDPE Injection Molding Applications:House waresThin-walled food containersPET bottle base cupInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® BB 85 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® FB 85 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® TB 38 HDPE Made for tape applications.Information provided by Unipetrol RPA |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D4883 |
ExxonMobil HD 6719.17 Injection Molding Resin Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ExxonMobil method |
ExxonMobil HDPE HD 6719.62 High Density Polyethylene Copolymer Resin Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D4883 |
ExxonMobil HDPE HPA 020 Molding High Density Polyethylene (HMW) Resin Product Description: HPA 020 is a high molecular weight HDPE resin, characterized by excellent balance of rigidity, ESCR and impact strength. Availability: Africa & Middle East, Asia Pacific and Eur.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D4883 |
ExxonMobil HDPE HPA 020 Wire & Cable High Density Polyethylene Resin Product Description: HPA 020 is a HDPE grade for Medium/High Voltage power cable jacketing. The grade should be used in blends with LLDPE to improve ESCR. Sufficient Carbon Black or UV stabilizer sh.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D792 |
Equate EPDA-5040 HDPE Non-Pressure Gravity Pipe Resin EPDA-5040 is a high molecular weight high density polyethylene copolymer resin designed for non-pressure gravity pipe applications. It has a good balance of flexibility, ductility, stiffness and tou.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | |
Dow DOWLEX™ IP-60 High Density Polyethylene DOWLEX® IP-60 resin is an improved processing high density polyethylene resin designed to offer excellent processability, good impact and top load strength required in thin wall injection molding. .. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D792 |
Dow UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE) Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6143 NT 7 is a polymer with broad molecular weight distri.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM-D792 |
Braskem GF5250 HDPE Blow Molding Polyethylene Copolymer GF5250 is a high-density polyethylene copolymer with well balanced properties between impact and stiffness combined with high productivity and good processability. It was developed for the blow-mold.. |
|||
Density | 0.952 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Amco PRIMATOP HDPE 003952 Phillips Process Hexene Copolymer HDPE 003952 features excellent stiffness and stress crack resistance properties. Applications include blow molding and sheet extrusion thermoforming.Former A-Top Polymers product; part of Amco produ.. |