BASF Ultradur B 4300 G2 High Speed Unc. 10% Glass Filled PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultradur B
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultradur B 4300 G2 High Speed Unc. 10% Glass Filled PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultradur B 4300 G2 High Speed Unc. is a high flow, fast cycling with low warpage, 10% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable applications.Applications: Housings, consoles, contact carriers, and covers.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Water Absorption 0.40 %
0.40 %
DIN 53495/1L
Moisture Absorption at Equilibrium 0.20 %
0.20 %
23°C/50% R.H.
Viscosity Test 100 cm³/g
100 cm³/g
Viscosity number; ISO 1628
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
60x60x2mm; ISO 294
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
60x60x2mm; ISO 294
Melt Flow 37.0 g/10 min

@Load 2.16 kg,
Temperature 250 °C
37.0 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 85.0 MPa
12300 psi
50mm/min; ISO 527-2
Elongation at Break 3.5 %
3.5 %
50mm/min; ISO 527
Modulus of Elasticity 4.40 GPa
638 ksi
ISO 527-2
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 - 225 °C
428 - 437 °F
Maximum Service Temperature, Air 210 °C
410 °F
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 162 °C
324 °F
ISO 75-2
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Comparative Tracking Index 300 V
300 V
Test solution A; IEC 60112
Processing Properties Metric English Comments
Melt Temperature 250 - 275 °C
482 - 527 °F
Injection molding
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Descriptive Properties Value Comments
Color Natural and Black
Commercial Status North America and Europe
Impact Modified No
Primary Processing Technique Injection Molding