Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
ISO 294-4
DSM Akulon® F223-DH (Dry) Low/Medium Viscosity, Heat Stabilized Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
DAM; ISO 294-4
DSM Akulon® F223-DH (Cond.) Low/Medium Viscosity, Heat Stabilized Nylon 6 (North America)  (discontinued **)&l
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
Injection molding; ISO 2577
Hexion Bakelite™ X22 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, mainly organically filled, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Pot handles, operating controls, electrical isolators, housing parts.Informati..
Linear Mold Shrinkage, Flow 0.0095 - 0.0125 cm/cm
0.0095 - 0.0125 in/in
LATI Latene® EP 7 TES/30 PP Copolymer, 30% Talc filled
Polypropylene copolymer (PPc) based compound. Aesthetic talc. Very good surface appearance. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo..
Linear Mold Shrinkage, Flow 0.0095 - 0.0125 cm/cm
0.0095 - 0.0125 in/in
LATI Latilub 62-10T PA6
Self-lubricating product based on Polyamide 6 (PA6). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..
Linear Mold Shrinkage, Flow 0.0095 - 0.0125 cm/cm
0.0095 - 0.0125 in/in
LATI Latilub 66 Y/20 PA66, Aramid Fiber Reinforced
Self-lubricating product based on Polyamide 66 (PA66). Aramid fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termo..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
Solvay TECHNYL® A 50H1 PA66, DRY
Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho..
Linear Mold Shrinkage, Flow 0.0095 - 0.011 cm/cm

@Thickness 3.20 mm
0.0095 - 0.011 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® X4820 PBT+PC
Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability.
Linear Mold Shrinkage, Flow 0.0095 - 0.011 cm/cm

@Thickness 3.20 mm
0.0095 - 0.011 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific)
Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability.
Linear Mold Shrinkage, Flow 0.0095 - 0.011 cm/cm

@Thickness 3.20 mm
0.0095 - 0.011 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East)
Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability.
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
DAM; ISO 294-4
DSM Akulon® F223-D Nylon 6 (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
DAM; ISO 294-4
DSM Akulon® F223-D Nylon 6 (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
ISO 294-4
DSM Akulon® F223-D Nylon 6 (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
ISO 294-4
DSM Akulon® F-X9183 PA6
Low/Medium Viscosity
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
ISO 294-4
DSM Akulon® S223-D (Dry) Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
DAM; ISO 294-4
DSM Akulon® S223-D Nylon 66 (European Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
DAM; ISO 294-4
DSM Akulon® S223-D Nylon 66 (European Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
ISO 294-4
DSM Akulon® S223-D Nylon 66 (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
DAM; ISO 294-4
DSM Akulon® S223-DH Nylon 66 (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
DAM; ISO 294-4
DSM Akulon® S223-DH Nylon 66 (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
ISO 294-4
DSM Akulon® S223-DH Nylon 66 (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
DAM; ISO 294-4
DSM Akulon® S223-DK Nylon 66 (European Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
DAM; ISO 294-4
DSM Akulon® S223-DK Nylon 66 (European Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Linear Mold Shrinkage, Flow 0.0095 - 0.0135 cm/cm
0.0095 - 0.0135 in/in
on Tensile Bar; E2P method
Eurostar Staramide BG2ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG2ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
ISO 294-4
DSM Akulon® S223-DK Nylon 66 (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
DAM; ISO 294-4
DSM Akulon® S223-D (Cond.) Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
DAM; ISO 294-4
DSM Akulon® F223-DH Nylon 6 (European Grade) (Cond)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
DAM; ISO 294-4
DSM Akulon® F223-DH Nylon 6 (European Grade) (Cond)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
ISO 294-4
DSM Akulon® F223-DH Nylon 6 (European Grade) (Dry)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Linear Mold Shrinkage, Flow 0.0095 cm/cm
0.0095 in/in
60x60x2mm; ISO 294
BASF Ultradur B 4300 G2 High Speed Unc. 10% Glass Filled PBT
Ultradur B 4300 G2 High Speed Unc. is a high flow, fast cycling with low warpage, 10% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable ap..