Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 222.1 g/mol
222.1 g/mol
Descriptive Properties Value Comments
CAS Number 304675-64-7
Form White powder
Purity 99.99+%
Typical Impurities Check with Manufacturer