Ashley Polymers Ashlene® 1430 Polycarbonate, 30% Glass Reinforced

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 30% Glass Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 1430 Polycarbonate, 30% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 30% glass reinforced polycarbonate for increased mechanical strength and thermal properties. Also available with UV stabilizer. 1433: with UV stabilizer; 1433-H2: with improved UV stabilizer.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Water Absorption 0.26 %
0.26 %
ASTM D570
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 117 MPa
17000 psi
ATSM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 6.60 GPa
957 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 141 °C
286 °F
ASTM D648