Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 4.40 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 4.40 GPa
638 ksi
Lehmann & Voss LUVOCOM® 3-8363 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
Modulus of Elasticity 4.40 GPa
638 ksi
Toyobo ECOVYLOPET® EMC2301 PET Bottle Recycling Grade, 15% Filler Reinforced
Features: PET Bottle Recycling Grade, 15% Filler Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.
Modulus of Elasticity 4.40 GPa
638 ksi
ASTM D638
Performance Polymers IPS II PPL-C1050 PEKK (Polyetherketoneketone) Linear Extrusion Grade
Amber pellets; neat resinInformation provided by Infinite Polymer System II.
Modulus of Elasticity 4.40 GPa
638 ksi
ASTM D638
Performance Polymers IPS II PPL-C4050 PEKK (Polyetherketoneketone) Linear Molding Grade
Amber pellets; neat resinInformation provided by Infinite Polymer System II.
Modulus of Elasticity 4.40 GPa
638 ksi
ISO 527-2
BASF Ultradur B 4300 G2 High Speed Unc. 10% Glass Filled PBT
Ultradur B 4300 G2 High Speed Unc. is a high flow, fast cycling with low warpage, 10% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable ap..