Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | ISO 294-4 |
DSM Akulon® F223-DH (Dry) Low/Medium Viscosity, Heat Stabilized Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | DAM; ISO 294-4 |
DSM Akulon® F223-DH (Cond.) Low/Medium Viscosity, Heat Stabilized Nylon 6 (North America)
(discontinued **)&l Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | Injection molding; ISO 2577 |
Hexion Bakelite™ X22 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Pot handles, operating controls, electrical isolators, housing parts.Informati.. |
|||
Linear Mold Shrinkage, Flow | 0.0095 - 0.0125 cm/cm | 0.0095 - 0.0125 in/in | |
LATI Latene® EP 7 TES/30 PP Copolymer, 30% Talc filled Polypropylene copolymer (PPc) based compound. Aesthetic talc. Very good surface appearance. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo.. |
|||
Linear Mold Shrinkage, Flow | 0.0095 - 0.0125 cm/cm | 0.0095 - 0.0125 in/in | |
LATI Latilub 62-10T PA6 Self-lubricating product based on Polyamide 6 (PA6). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Linear Mold Shrinkage, Flow | 0.0095 - 0.0125 cm/cm | 0.0095 - 0.0125 in/in | |
LATI Latilub 66 Y/20 PA66, Aramid Fiber Reinforced Self-lubricating product based on Polyamide 66 (PA66). Aramid fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termo.. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | |
Solvay TECHNYL® A 50H1 PA66, DRY Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho.. |
|||
Linear Mold Shrinkage, Flow | 0.0095 - 0.011 cm/cm @Thickness 3.20 mm |
0.0095 - 0.011 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Linear Mold Shrinkage, Flow | 0.0095 - 0.011 cm/cm @Thickness 3.20 mm |
0.0095 - 0.011 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Linear Mold Shrinkage, Flow | 0.0095 - 0.011 cm/cm @Thickness 3.20 mm |
0.0095 - 0.011 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | DAM; ISO 294-4 |
DSM Akulon® F223-D Nylon 6 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | DAM; ISO 294-4 |
DSM Akulon® F223-D Nylon 6 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | ISO 294-4 |
DSM Akulon® F223-D Nylon 6 (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | ISO 294-4 |
DSM Akulon® F-X9183 PA6 Low/Medium Viscosity |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | ISO 294-4 |
DSM Akulon® S223-D (Dry) Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | DAM; ISO 294-4 |
DSM Akulon® S223-D Nylon 66 (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | DAM; ISO 294-4 |
DSM Akulon® S223-D Nylon 66 (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | ISO 294-4 |
DSM Akulon® S223-D Nylon 66 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | DAM; ISO 294-4 |
DSM Akulon® S223-DH Nylon 66 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | DAM; ISO 294-4 |
DSM Akulon® S223-DH Nylon 66 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | ISO 294-4 |
DSM Akulon® S223-DH Nylon 66 (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | DAM; ISO 294-4 |
DSM Akulon® S223-DK Nylon 66 (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | DAM; ISO 294-4 |
DSM Akulon® S223-DK Nylon 66 (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0095 - 0.0135 cm/cm | 0.0095 - 0.0135 in/in | on Tensile Bar; E2P method |
Eurostar Staramide BG2ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG2ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | ISO 294-4 |
DSM Akulon® S223-DK Nylon 66 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | DAM; ISO 294-4 |
DSM Akulon® S223-D (Cond.) Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | DAM; ISO 294-4 |
DSM Akulon® F223-DH Nylon 6 (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | DAM; ISO 294-4 |
DSM Akulon® F223-DH Nylon 6 (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | ISO 294-4 |
DSM Akulon® F223-DH Nylon 6 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Linear Mold Shrinkage, Flow | 0.0095 cm/cm | 0.0095 in/in | 60x60x2mm; ISO 294 |
BASF Ultradur B 4300 G2 High Speed Unc. 10% Glass Filled PBT Ultradur B 4300 G2 High Speed Unc. is a high flow, fast cycling with low warpage, 10% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable ap.. |