Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 265 - 275 °C | 509 - 527 °F | |
Celanese Celanex® 2302 GV1/30 PBT, 30% Glass Reinforced
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: PBT30% glass fiber reinforced, high glossInformation provided by Celanese |
|||
Melt Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact Feature: Injection Molding, PA6/ABS+MF6%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
Melt Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
Melt Temperature | 245 - 275 °C | 473 - 527 °F | Injection Molding |
LG Chemical LUPOY GN5151RFA PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9, 181028-79-5 an.. |
|||
Melt Temperature | 255 - 275 °C | 491 - 527 °F | |
MRC Polymers NAXALOYâ„¢ 780 GF11 PC+PBT Polyester Blend, 11% Glass Fiber Filled Good chemical resistance, impact and heat resistanceAvailable in Black OnlyCan be UV StabilizedInternal and external lubricant can be added.Information provided by MRC Polymers Inc. |
|||
Melt Temperature | 210 - 275 °C | 410 - 527 °F | |
Borealis MG7547B Polyethylene MG7547B is a high-density polyethylene produced by a low pressure process. This grade has an excellent impact strength and low distortion even at low temperatures. It also contains UV stabilizer, wh.. |
|||
Melt Temperature | 240 - 275 °C | 464 - 527 °F | |
A. Schulman SCHULAMID® 6 MV5 Unreinforced Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 240 - 275 °C | 464 - 527 °F | |
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 240 - 275 °C | 464 - 527 °F | |
A. Schulman SCHULAMID® 6 MV5 Unreinforced Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 260 - 275 °C | 500 - 527 °F | |
CP-Polymer-Technik Wellamid® 6600 PA-66-HWV0CP UL-Licensed Nylon 66, Flame Protection, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 265 - 275 °C | 509 - 527 °F | |
Eurostar Staramide 6 70E3 PA6, 70% Mineral Filled, Injection Molded Staramide 6 70E3 is a 70% mineral filled high density, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 265 - 275 °C | 509 - 527 °F | |
Eurostar Staramide AST43 PA66, Impact Modified, Injection Molded AST43 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Melt Temperature | 265 - 275 °C | 509 - 527 °F | |
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Melt Temperature | 265 - 275 °C | 509 - 527 °F | |
Eurostar Staramide PB00A PA6, 50% Glass Bead Filled, Injection Molded Staramide PB00A is a 50% Glass Bead Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 265 - 275 °C | 509 - 527 °F | |
Eurostar Staramide RF004EU PA66/6, 20% Glass Fiber Filled, Injection Molded Staramide RF004EU is a 20% Glass Fiber Reinforced Polyamide 66/6 Injection Molding (also known as Staramide 66C 20V S4)Information provided by Eurostar. |
|||
Melt Temperature | 265 - 275 °C | 509 - 527 °F | |
Eurostar Starflam RX06082 PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Staramide RX06082 is a Halogen Free and Red Phosphorous Free, flame Retardant, Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 265 - 275 °C | 509 - 527 °F | |
Eurostar Staramide RF006EU PA66/6, Glass Fiber Filled, Injection Molded Staramide RF006EU is an UV stabilized, Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66C 30V S4)Information provided by Eurostar. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | |
BASF Ultradur B 4040 G6 High Speed BK15029 30% Glass Filled PBT/PET Ultradur B 4040 G6 High Speed BK15029 is a high flow, fast cycling with low warpage, 30% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection molding |
BASF Ultradur B 4300 G2 10% Glass Filled PBT Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection-molding |
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT Description: Is a PBT-HI, injection-molding grade reinforced with 25% of minerals, for the production of parts with good surface quality and low warpage, e.g. housings and visible parts of domestic .. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection molding/Extrusion |
BASF Ultradur® B 4520 High Speed PBT Description: Very easy flowing unreinforced injection molding grade with enhanced elongation for thin-walled parts (e.g. automotive connectors, switches, relay parts)Information provided by BASF |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection-molding |
BASF Ultradur® S 4090 GM11 5/5% Glass/Mineral Filled PBT Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber/mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventilation gri.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection-molding/Extrusion |
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection-molding/Extrusion |
BASF Ultramid® FRee B3U31G4 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection molding |
BASF Ultradur B 4406 G4 PBT Description: Is a PBT, flame-retardant injection-molding grades, with 20% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection-molding |
BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET Description: Is a PBT + PET, injection-molding grade containing 10% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, .. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection-molding |
BASF Ultradur® B 4300 GM42 20/10% Glass/Mineral Filled PBT Description: Is a PBT-HI, mixed glass-fiber-reinforced and mineral-reinforced injection-molding grade with good surface quality and rigidity, and with low warpage for parts such as housings and PCBs.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection-molding |
BASF Ultradur® B 4300 M2 12.5% Mineral Filled PBT Description: Is a PBT-HI, mineral-reinforced, impact-modified injection-molding grade for rigid parts, for example automotive power door locks.Information provided by BASF |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection-molding |
BASF Ultradur® S 4090 G6 High Speed 30% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 30% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers.. |
|||
Melt Temperature | 250 - 275 °C | 482 - 527 °F | Injection-molding |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |