Polymer Property : Melt Temperature = 527 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 220 - 275 °C
428 - 527 °F
Ovation Polymers Nemcon™ H ABS DP116P ABS
ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers
Melt Temperature 255 - 275 °C
491 - 527 °F
Start Point: 260°C
Kingfa PET-RG20 Flame Retardant, 20% Glass Fiber Reinforced PET
Features:Flame retardantHigh strengthGood heat resistanceOutstanding electrical propertiesApplications:Injection moldingConnectorsRelayBobbinsSocketsE & E partsInformation Provided by Kingfa Sci. & ..
Melt Temperature 255 - 275 °C
491 - 527 °F
Start Point: 260°C
Kingfa PET-RG30 Flame Retardant, 30% Glass Fiber Reinforced PET
Features:Flame retardantHigh strengthGood heat resistanceOutstanding electrical propertiesApplications:Injection moldingConnectorsRelayBobbinsSocketsE & E partsInformation Provided by Kingfa Sci. & ..
Melt Temperature 270 - 275 °C
518 - 527 °F
Injection Molding
LG Chemical LUMID GP3200B(W) PA66+MF20%, General Purpose
Feature: Injection Molding, PA6+MF20%, General PurposeApplication: E&E (Rice Cooker Housing)Information provided by LG Chemical
Melt Temperature 245 - 275 °C
473 - 527 °F
Injection Molding
LG Chemical LUPOY GN5151RFA PC/ABS Mineral Filler
Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9, 181028-79-5 an..
Melt Temperature 250 - 275 °C
482 - 527 °F
Injection Molding
LG Chemical LUPOY GP5006BH PC/ABS, Heat Resistance, Impact Strength
Description: Injection Molding, PC/ABS, Heat Resistance, Impact Strength, High ToughnessApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical..
Melt Temperature 260 - 275 °C
500 - 527 °F
Lavergne VYPET VNT 1020 Polyester-PC Alloy
The Vypet 1020 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic..
Melt Temperature 265 - 275 °C
509 - 527 °F
Lavergne VYTEEN PC/ABS 8515XF Polycarbonate - Acrylonitrile Butadiene Styrene Alloy
Vyteen PC/ABS 8515XF is an enhanced PC/ABS alloy with balanced impact/stiffness properties designed for injection molding applications.Features: -High resilience -Excellent processability -High d..
Melt Temperature 255 - 275 °C
491 - 527 °F
Start Point: 260°C
Kingfa PET-G30 30% Glass Fiber Reinforced PET
Features:High strengthGood heat resistanceApplications:Injection moldingApplication partsAuto partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Melt Temperature 210 - 275 °C
410 - 527 °F
Borealis MG7547S Polyethylene
MG7547S is a high-density polyethylene produced by a low pressure process. This grade has an excellent impact strength and low distortion even at low temperatures. It also contains UV stabilizer, wh..
Melt Temperature 210 - 275 °C
410 - 527 °F
Borealis MG9647B Polyethylene
MG9647B is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of..
Melt Temperature 240 - 275 °C
464 - 527 °F
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6
Information provided by A. Schulman.
Melt Temperature 240 - 275 °C
464 - 527 °F
A. Schulman SCHULAMID® 6 MV5 Unreinforced Nylon 6
Information provided by A. Schulman.
Melt Temperature 240 - 275 °C
464 - 527 °F
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6
Information provided by A. Schulman.
Melt Temperature 240 - 275 °C
464 - 527 °F
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6
Information provided by A. Schulman.
Melt Temperature 240 - 275 °C
464 - 527 °F
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6
Information provided by A. Schulman.
Melt Temperature 265 - 275 °C
509 - 527 °F
Eurostar Staramide 6 70E3 PA6, 70% Mineral Filled, Injection Molded
Staramide 6 70E3 is a 70% mineral filled high density, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Melt Temperature 265 - 275 °C
509 - 527 °F
Eurostar Staramide AST43 PA66, Impact Modified, Injection Molded
AST43 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Melt Temperature 265 - 275 °C
509 - 527 °F
Eurostar Staramide R1000K PA66, Injection Molded
Staramide R1000K is an Unreinforced Radiation Crosslinkable Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Melt Temperature 250 - 275 °C
482 - 527 °F
Injection molding
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT
Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle..
Melt Temperature 250 - 275 °C
482 - 527 °F
Injection-molding
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT
Description: Is a PBT-HI, injection-molding grade reinforced with 25% of minerals, for the production of parts with good surface quality and low warpage, e.g. housings and visible parts of domestic ..
Melt Temperature 250 - 275 °C
482 - 527 °F
Injection-molding/Extrusion
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Conditioned)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Melt Temperature 250 - 275 °C
482 - 527 °F
Injection-molding/Extrusion
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Dry)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Melt Temperature 250 - 275 °C
482 - 527 °F
Injection molding
BASF Ultradur B 4406 G4 PBT
Description: Is a PBT, flame-retardant injection-molding grades, with 20% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh..
Melt Temperature 250 - 275 °C
482 - 527 °F
Injection molding
BASF Ultradur S 4090 G4 20% Glass Filled PBT
Ultradur S 4090 G4 is a 20% glass reinforced PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicatio..
Melt Temperature 240 - 275 °C
464 - 527 °F
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6
Information provided by A. Schulman.
Melt Temperature 240 - 275 °C
464 - 527 °F
A. Schulman SCHULAMID® 6 MV5 Unreinforced Nylon 6
Information provided by A. Schulman.
Melt Temperature 235 - 275 °C
455 - 527 °F
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, DAM
Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced ..
Melt Temperature 250 - 275 °C
482 - 527 °F
Injection-molding
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT
Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit..
Melt Temperature 250 - 275 °C
482 - 527 °F
Injection molding/Extrusion
BASF Ultradur® B 4300 G4 FC 20% Glass Filled PBT
Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation..