Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | >= 210 °C | >= 410 °F | pending UL RTI |
Rogers Corporation XT/duroid™ 8100 0.004" Woven Glass Reinforced Thermoplastic Circuit Material XT/duroid™ 8100 woven glass reinforced thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 81.. |
|||
Maximum Service Temperature, Air | 210 °C @Time 5.40e+6 sec |
410 °F @Time 1500 hour |
Continuous; ASTM D3045 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | short term |
Lehmann & Voss LUVOCOM® 3/CF/30 Polyamide 6, with carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable.. |
|||
Maximum Service Temperature, Air | 210 - 230 °C | 410 - 446 °F | Softening Range |
Huntsman DT 3368 Matting Agent Color: Off-whiteComments/Applications: Reactive matting agent for very low gloss epoxy and epoxy/polyester hybrid powder formulations.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemica.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
Greene Tweed CHEMRAZ® 571 Perfluoroelastomer Chemraz® 571 is recommended for a wide variety of semiconductor equipment wet processing applications where stringent seal reliability and contamination control are required. This seal material .. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | Heat Resistance; DIN 53772 |
Karina 4000/35-IE MBPEBD Green Color Concentrate Color concentrate recommended for polyolefin applications and 2% minimum adding.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
Glastic Laminates/Shapes SG-200 Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Excellent thermal endurance - used to replace silicone rod. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | < 50 hours; IEC 60216-P1 |
Hexion UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability, very slight post shrinkage, good mechanical properties, increased electrical value.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | Continuous Use |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | 50 Minutes; EN 728 |
Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide)) BorPEX HE2557 is a yellow, high molecular weight, high density polyethylene compound for crosslinkable pipes, specially designed for peroxide crosslinking. Long term stability and UV resistance is .. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | few hours; VDE 0304/P2-1, IEC 216 |
EPICHEM Epinyl PA 66 GF 30 H Polyamide 66, 30% Glass, Heat Stabilized Characteristics: 30% glass fibre filled |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
Epoxyset Epoxibond EB-315 Low Expansion Epoxy Adhesive EB-315 is a highly filled, heat curing, high temperature resistant epoxy adhesive. Due to its low coefficient of thermal expansion and outgassing, it can be used for bonding and sealing in critical .. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
Elisto THERMOSTAR® XPS Mold Insulation Material Lateral insulationInformation provided by elisto |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | Martens Dimensional Stability |
CMT Materials METAPOR® HD 210 AL Air Permeable Material METAPOR® is a composite material made of aluminum granules and epoxy resin. The material is air-permeable over the entire surface due to its micro-porous structure allowing for unique design consi.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur B 4040 G6 High Speed BK15029 30% Glass Filled PBT/PET Ultradur B 4040 G6 High Speed BK15029 is a high flow, fast cycling with low warpage, 30% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4300 G6 HR 30% Glass Filled PBT Description: Is a PBT, injection-molding grade with 30% glass fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance, e.g. automotive connect.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | Long Term |
CENTROPLAST CENTROTRON GF 40 Polyphenylene sulfide 40% glass fiber CENTROTRON GF is a plastic that is reinforced for high strength and rigidity, that can be used at high operating temperatures. Applications include bearings, sealing rings, rods and hollow bars. In.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur B 4406 G4 PBT Description: Is a PBT, flame-retardant injection-molding grades, with 20% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled PBT Description: Is a PBT, easy-flowing injection-molding grades with 15% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers, cove.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4406 G2 10% Glass Filled PBT Description: Is a PBT, flame-retardant injection-molding grades, with 10% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4406 G6 30% Glass Filled PBT Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur B 4300 G2 High Speed Unc. 10% Glass Filled PBT Ultradur B 4300 G2 High Speed Unc. is a high flow, fast cycling with low warpage, 10% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable ap.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | ASTM D794 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |
|||
Maximum Service Temperature, Air | 210 °C @Time 4.32e+6 sec |
410 °F @Time 1200 hour |
Continuous; ASTM D3045 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 20% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4300 G2 FC 10% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Maximum Service Temperature, Air | 210 °C | 410 °F | |
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT Description: Easy flowing injection molding grade with 30 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg windshield wiper arms, printed circuit boards PCBs), housing, .. |