Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast/AboCure 8501-4/8501-4 High Temperature Resistant Epoxy

Category Polymer , Thermoset , Epoxy , Epoxy, Cast, Unreinforced , Epoxy, High Temperature
Manufacturer Abatron
Trade Name AboCast/AboCure
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast/AboCure 8501-4/8501-4 High Temperature Resistant Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Gray, high viscosity, structural/machinable epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components to be used at temperatures up to 300°C. Casting and assembly of tools, patterns, models and structural components that must operate in extremely hot and corrosive environments.Processing: 100/41 ratio (pbw). Cured 2 hours at 95°C + 24 hour post-cure at 260°C. Information provided by Abatron.
Physical Properties Metric English Comments
Viscosity 30000 cP

@Temperature 25.0 °C
30000 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Thermal Conductivity 0.586 - 0.795 W/m-K
4.06 - 5.51 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 300 °C
572 °F
Processing Properties Metric English Comments
Pot Life 1200 min

@Temperature 25.0 °C
1200 min

@Temperature 77.0 °F
Users viewing this material also viewed the following: