Material Notes:
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent characteristics and similar properties of PTFE but can be processed using conventional thermoplastic techniques, such as extrusion molding, injection molding, blow molding, or electrostatic powder coating. And Fluon® PFA can be used in a wide range of temperatures from extremely low to high temperatures (260°C at the maximum) without losing its superior properties. Information provided by Asahi Glass Company, Inc.
Physical Properties Metric English Comments
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ASTM D792
Water Absorption <= 0.030 %
<= 0.030 %
ASTM D570
Melt Flow 1.0 - 3.0 g/10 min
1.0 - 3.0 g/10 min
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D1706
Tensile Strength at Break 39.0 MPa
5660 psi
ASTM D638
Tensile Strength, Ultimate 17.0 MPa

@Temperature 250 °C
2470 psi

@Temperature 482 °F
ASTM D638
Elongation at Break 340 %
340 %
ASTM D638
740 %

@Temperature 250 °C
740 %

@Temperature 482 °F
ASTM D638
Flexural Modulus 0.540 GPa
78.3 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256A
Coefficient of Friction, Dynamic 0.20
0.20
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C

@Temperature 20.0 °C
72.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.046 J/g-°C
0.2500 BTU/lb-°F
Thermal Conductivity 0.251 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 305 - 315 °C
581 - 599 °F
Maximum Service Temperature, Air 260 °C
500 °F
Continuous
Flammability, UL94 V-0
V-0
Oxygen Index >= 95 %
>= 95 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+18 ohm-cm
>= 1.00e+18 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+17 ohm
>= 1.00e+17 ohm
ASTM D257
Dielectric Constant <= 2.1

@Frequency 60 Hz
<= 2.1

@Frequency 60 Hz
ASTM D150
<= 2.1

@Frequency 1000 Hz
<= 2.1

@Frequency 1000 Hz
ASTM D150
<= 2.1

@Frequency 1e+6 Hz
<= 2.1

@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor <= 0.00020

@Frequency 60 Hz
<= 0.00020

@Frequency 60 Hz
ASTM D150
<= 0.00020

@Frequency 1000 Hz
<= 0.00020

@Frequency 1000 Hz
ASTM D150
<= 0.00020

@Frequency 1e+6 Hz
<= 0.00020

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 300 sec
>= 300 sec
ASTM D495
Descriptive Properties Value Comments
Ball Pressure Temperature, °C 230
Flex Life, Cycles 500000