Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Europe-Africa-Middle East) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Surface Resistance | 1.00e+17 ohm @Temperature 23.0 °C |
1.00e+17 ohm @Temperature 73.4 °F |
IEC 60093 |
DuPont Performance Polymers Crastin® HR5315HF BK503 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | insulation resistance |
NOVA Chemicals Sclair® 35BE HDPE Extrusion Resin
(discontinued **) Features: Medium molecular weight HDPE, excellent ESCR, excellent toughness, good processability, outstanding abrasion resistance.Applications: Extrusion on to metal pipes to produce a corrosion res.. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Asia Pacific) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
3M Dyneon™ TF 2024 PTFE Paste Extrusion Powder
(discontinued **) Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 500. Average particle size 500µm. Used for unsintered tapes and sealing cords.Dyneon offers a family of PTFE fine powder .. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s.. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
Solvay Specialty Polymers Hyflon® PFA P455 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
Techmer ES HiFill FR® PC FR SFX-ORANGE 1.0 Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantAppearance: OrangeInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM3020 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_FM3020 compound is GR/MR 30%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM3020 PPE+PS LNP* Thermocomp* Noryl_FM3020 compound is GR/MR 30%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
Cosmic Plastics 306 Orlon Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
Dalau Dalcon 086 100% Virgin PTFE modified polymer Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal .. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
Cosmic Plastics D72 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
Polyplastics Duranex® 701SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
Polyplastics FR-PET® B3015FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
Covestro Bayblend® FR3040 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
Cosmic Plastics 6120F Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | Average value: 1.00e+17 ohm Grade Count:4 |
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma.. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
Cosmic Plastics 6120 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |