Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
ISO 11359-2
Celanese Vandar® 2100 PBT  (Unverified Data**)
Vandar 2100 is a polyester alloy designed to offer maximum impact strength at room and low temperatures. This unfilled compound is characterized by outstanding chemical resistance, dimensional stabi..
CTE, linear 130 - 160 µm/m-°C

@Temperature 20.0 °C
72.2 - 88.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer  (discontinued **)
Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i..
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
Above Tg
EVALCA EVAL® LC-E105A Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
44 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, melt phase forming, solid phase pressure forming, tubes, coex coating. EVOH is used in packaging applications because of its out..
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
Above Tg
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas..
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
Above Tg
EVALCA EVAL® G110 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
48 mol % Ethylene.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of the Kuraray product line.
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
ASTM D696
Kolon KOCETAL® CB301 Conductive Grade Acetal Resin
Conductive grade. Applications: Conductive products. Information provided by API-Kolon.
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
ASTM D696
Kolon KOCETAL® DS500 Acid Resistant Acetal Resin
Improved acid resistance. Applications: Products for improved chemical resistance. Information provided by API-Kolon.
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
ASTM D696
Kolon KOCETAL® EL302 Toughened Grade Acetal Resin
Flexible grade. Applications: Flexible products. Information provided by API-Kolon.
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
ASTM D696
Kolon KOCETAL® EL304 Toughened Grade Acetal Resin
Flexible grade. Applications: Flexible products. Information provided by API-Kolon.
CTE, linear 130 µm/m-°C

@Temperature 20.0 - 100 °C
72.2 µin/in-°F

@Temperature 68.0 - 212 °F
Isoflon PFA Polyperfluoroalkoxyethylene
Fluoropolymer material specifications.Information provided by Isoflon.
CTE, linear 130 µm/m-°C

@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duracon® AW-01 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
Above Tg
Tra-Con Tra-Bond 342-14T Low Viscosity Room Temperature Cure Epoxy Adhesive
TRA-BOND 342-14T single component, low viscosity alumina-filled epoxy adhesive exhibits high bond strength and excellent thermal shock characteristics. This adhesive may be cured at room temperature..
CTE, linear 130 µm/m-°C

@Temperature 20.0 °C
72.2 µin/in-°F

@Temperature 68.0 °F
Tra-Con Tra-Bond F175T One-Part Thixotropic UV Curing Adhesive
TRA-BOND F175T is a thixotropic, one part UV curing adhesive designed for bonding metals, ceramics and most rigid polymers. It is an excellent adhesive for fiber optic terminations where fast cure w..
CTE, linear 130 µm/m-°C

@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duracon® SF-15 Acetal Co-polymer (POM), High impact, Flexible
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® H77 Thermally Conductive Epoxy
Product Description: EPO-TEK® H77 is a two component, thermally conductive, electrically insulating epoxy system designed for lid-sealing of hybrids found in hermetic packaging of micro-electronics..
CTE, linear 130 - 150 µm/m-°C
72.2 - 83.3 µin/in-°F
Hippe PE 300 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
ISO 11359-2
Celanese Celanex® 3109HR PBT, 7.5% Glass Reinforced
Celanex 3109HR is a non-lubricated, 7.5% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties, and processability.7.5% glass filledInform..
CTE, linear 130 µm/m-°C

@Temperature 20.0 °C
72.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Glass Fluon® P-66P PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
CTE, linear 130 µm/m-°C

@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 131 °F
Longitudinal, 30x10x4 mm from multi-purpose test specimen (ISO 3167); ISO 11359, part 1/2
Celanese Hostaform® S 9244 Impact Grade Acetal Copolymer
Description: Hostaform® Acetal Copolymers are a high strength, crystalline, thermoplastic engineering resins whose balance of properties and ease of processability offer performance and cost advant..
CTE, linear 130 µm/m-°C

@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 131 °F
Longitudinal, 30x10x4 mm from multi-purpose test specimen (ISO 3167); ISO 11359, part 1/2
Celanese Hostaform® T 1020 Extrusion Blow Molding Grade Acetal Copolymer
Description: Hostaform® Acetal Copolymers are a high strength, crystalline, thermoplastic engineering resins whose balance of properties and ease of processability offer performance and cost advant..
CTE, linear 130 µm/m-°C

@Temperature -30.0 - 100 °C
72.2 µin/in-°F

@Temperature -22.0 - 212 °F
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive
3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa..
CTE, linear 130 µm/m-°C

@Temperature 20.0 °C
72.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Glass Fluon® P-62XP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
CTE, linear 130 µm/m-°C

@Temperature 20.0 °C
72.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Glass Fluon® P-830UP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
Hippe PVDF
Better mechanical strength compared to other fluorinated polymers. Tough and hard. High-grade electrical feature. Good weathering stability. Physiologically safe. Not as good as fluorinated pol..
CTE, linear 130 µm/m-°C

@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duracon® HP25X Acetal Co-polymer (POM), High stiffness, High viscosity
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
CTE, linear 130 µm/m-°C

@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duracon® TD-20 Acetal Co-polymer (POM), High impact, Flexible
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Copyright © lookpolymers.com All Rights Reserved